Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 131 MPa | 19000 psi | ASTM D790 |
NYCOA 2038 10% Glass Filled Nylon 6 10% glass filled very high viscosity nylon 6Information provided by NYCOA, Inc. |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | ASTM D790 |
Chevron Phillips Ryton® R10 5004A PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Flexural Yield Strength | 131 MPa @Thickness 3.17 mm |
19000 psi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-20GFR 20% Glass Reinforced Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | ASTM D790 |
Techmer ES Electrafil® J-50/CF/10/TF/13/SI/2 Polycarbonate, 10% Carbon Fiber Reinforced, 13% PTFE, 2% Silicone |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® 1760 PBT+PC 11% Glass Reinforced PBT+PC alloy. Impact/chemical resistant. Excellent physical property retention in automotive exteriors. |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | ASTM D790 |
Techmer ES HiFill® PP G/CF40 CC 40% Glass/Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Carbon Fiber Reinforcement, 40% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | ASTM D790 |
Sumitomo Bakelite North America RX® 3-1-525F-P Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG-F.I.. |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL LTA1350 PPE+PS Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Asia Pacific) Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | ASTM D790 |
Techmer ES Electrafil® J-50/CF/10/TF/15 Polycarbonate, 10% Carbon Fiber Reinforced, 15% PTFE |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | ASTM D790 |
Sumitomo Bakelite North America 52-20-30 Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ.. |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Europe-Africa-Middle East) Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | ASTM D790 |
Westlake Plastics Zelux® 20% GF Polycarbonate 20% Glass Filled Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and .. |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | ASTM D790 |
Clariant Renol 66B40 Nylon 66, 40% Glass Bead Filled Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | |
Abatron AboCast/AboCure 8109-2 High melting point. Filled version.Processing: 100/10 pbw; 90 minute potlife; mix at 130-140°C (270 °F); cures in 16 h/120°C (250°F), 10 h/140°C (285°F), 8 h/160°C (320°F), 2 h/ 200°C (390°.. |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | ASTM D790 |
Chem Polymer Formax 630 G Acetal, 30% Glass Fiber Reinforced A copolymer acetal reinforced with 30% glass fiber for use in applications requiring great strength and rigidity.Data provided by the manufacturer, Chem Polymer. |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 3412R PC 20% GR, provides improved mechanical properties and UL94 V-1 rated at 0.058"". Internal mold release added. |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | ASTM D790 |
Custom Resins Norpex® GF3 PPE (Polyphenylene Ether), 30% Glass Filled
(discontinued **) Properties for dry as molded samples.Data provided by the manufacturer |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | ASTM D790 |
Sumitomo Bakelite North America FS-4 Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North A.. |
|||
Flexural Yield Strength | 131 - 165 MPa | 19000 - 24000 psi | ASTM D790 |
Premix Premi-Glas® 1200-24 Polyester SMC
(discontinued **) Premi-Glas® 1200-24 is a 24% fiberglass-reinforced, thermoset, sheet molding compound designed for Class A Heavy Truck - Bus body panels and Marine cowls parts where smooth, flat, ripple free surfa.. |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | ASTM D790 |
Techmer ES HiFill® PVDF CF10 BK 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 10% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |