Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 221 - 283 MPa | 32000 - 41000 psi | ASTM D882 |
Honeywell Capran® Emblem™ 2530 Bi-Axially Oriented Nylon Film
(discontinued **) Description: Capran® Emblem™ 2530 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbo.. |
|||
Film Tensile Strength at Break, TD | 221 - 290 MPa | 32000 - 42000 psi | ASTM D882 |
Honeywell Capran® Emblem™ 1000 Bi-Axially Oriented Nylon 6 Film Description: Capran® Emblem™ 1000 is a 0.40 mil (10 micron) biaxially oriented nylon 5 film with excellent flex crack resistance and superior clarity properties. Applications: packaging appl.. |
|||
Film Tensile Strength at Break, TD | 221 - 283 MPa | 32000 - 41000 psi | ASTM D882 |
Honeywell Capran® Emblem™ 2500 Bi-Axially Oriented Nylon Film Description: Capran® Emblem™ 2500 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydr.. |
|||
Film Tensile Strength at Break, TD | 221 - 283 MPa | 32000 - 41000 psi | ASTM D882 |
Honeywell Capran® Emblem™ 2500M M-Coated Bi-Axially Oriented Nylon Film Description: Capran® Emblem™ 2500M is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hyd.. |
|||
Film Tensile Strength at Break, TD | 221 - 283 MPa | 32000 - 41000 psi | ASTM D882 |
Honeywell Capran® Emblem™ MT2500 Bi-Axially Oriented Nylon 6 Film Description: Capran® Emblem™ MT2500 is a 1.00 mil (25 micron) biaxially oriented nylon 6 film with a metallized barrier coating.Applications: Capron® Emblem™ MT2500 is well suited fo.. |
|||
Film Tensile Strength at Break, TD | 221 MPa | 32000 psi | ASTM D882A |
DuPont Teijin Films Melinex® SWC Polyester Film, 200 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Film Tensile Strength at Break, TD | 221 MPa | 32000 psi | ASTM D882A |
DuPont Teijin Films Melinex® SWC Polyester Film, 300 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Film Tensile Strength at Break, TD | 221 MPa | 32000 psi | ASTM D882A |
DuPont Teijin Films Melinex® SWC Polyester Film, 400 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Film Tensile Strength at Break, TD | 221 MPa | 32000 psi | ASTM D882A |
DuPont Teijin Films Melinex® SWC Polyester Film, 48 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Film Tensile Strength at Break, TD | 221 MPa | 32000 psi | ASTM D882A |
DuPont Teijin Films Melinex® SWC Polyester Film, 500 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Film Tensile Strength at Break, TD | 221 MPa | 32000 psi | ASTM D882A |
DuPont Teijin Films Melinex® SWC Polyester Film, 92 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Film Tensile Strength at Break, TD | 221 MPa | 32000 psi | ASTM D882A |
DuPont Teijin Films Melinex® XST6562 Polyester Film, 200 Gauge Melinex® XST6562 is a thermally stabilized high clarity polyester film with good handleability. It is pretreated on one film surface to promote adhesion.Information provided by DuPont. |
|||
Film Tensile Strength at Break, TD | 221 MPa | 32000 psi | ASTM D882A |
DuPont Teijin Films Mylar® DS Polyester Film Mylar® DS is a super clear, biaxially oriented, polyester film with differential surface roughness on each side. Its unique composition, consisting of a smooth side opposite a rougher, filled side,.. |
|||
Film Tensile Strength at Break, TD | 221 MPa | 32000 psi | ASTM D882A |
DuPont Teijin Films Mylar® EL Polyester Film, 48 Gauge Mylar® EL films, typically 48 through 500 gauge are strong, tough, general -purpose films for electrical/electronic uses. Heavier gauges of Mylar® EL films are similar to Mylar® MO films. Availab.. |
|||
Film Tensile Strength at Break, TD | 221 MPa | 32000 psi | ASTM D882A |
DuPont Teijin Films Mylar® WC Polyester Film, 48 Gauge Mylar® WC films are general-purpose electrical grade films, similar to Mylar® EL. These clear to hazy films are tough and durable as a core wrap. They offer good dielectrics and good handling char.. |
|||
Film Tensile Strength at Break, TD | 221 MPa | 32000 psi | ASTM D882A |
DuPont Teijin Films Mylar® WRL63 Polyester Film, 200 Gauge Mylar® WRL63 is a biaxially oriented polyester (OPET) film with a modified ethylene acrylate heat seal layer. It provides peelable seal over a broad temperature range to a number of bottles or cont.. |
|||
Film Tensile Strength at Break, TD | 221 MPa | 32000 psi | ASTM D882A |
DuPont Teijin Films Teijin® Tetoron® SL Polyester Film, 200 Gauge Teijin® Tetoron® SL is a low shrinkage version of Teijin® Tetoron® type S polyester film. In addition to having the well balanced physical, chemical and electrical properties of type S film, Tei.. |
|||
Film Tensile Strength at Break, TD | 221 MPa | 32000 psi | ASTM D882A |
DuPont Teijin Films Teijin® Tetoron® SL Polyester Film, 300 Gauge Teijin® Tetoron® SL is a low shrinkage version of Teijin® Tetoron® type S polyester film. In addition to having the well balanced physical, chemical and electrical properties of type S film, Tei.. |
|||
Film Tensile Strength at Break, TD | 221 MPa | 32000 psi | ASTM D882A |
DuPont Teijin Films Teijin® Tetoron® SLA Polyester Film, 200 Gauge Teijin® Tetoron® SLA is a super low shrinkage version of Teijin® Tetoron® type S polyester film. In addition to having the well balanced physical, chemical and electrical properties of type S fi.. |
|||
Film Tensile Strength at Break, TD | 221 MPa | 32000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor® 70 PXS OPP Film Product Description: Bicor PXS is one-side sealable, PVdC-coated OPP film designed for use as the inside sealant web in laminations.Availability: Latin America, North America and South AmericaKey Fe.. |
|||
Film Tensile Strength at Break, TD | 221 MPa | 32000 psi | ASTM D882A |
DuPont Teijin Films Mylar® A Polyester Film, 48 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Film Tensile Strength at Break, TD | 221 MPa | 32000 psi | ASTM D882A |
DuPont Teijin Films Mylar® MDA Polyester Film, 48 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Film Tensile Strength at Break, TD | 221 MPa | 32000 psi | ASTM D882A |
DuPont Teijin Films Teijin® Tetoron® SL Polyester Film, 500 Gauge Teijin® Tetoron® SL is a low shrinkage version of Teijin® Tetoron® type S polyester film. In addition to having the well balanced physical, chemical and electrical properties of type S film, Tei.. |