Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Teijin Films Melinex® XST6562 Polyester Film, 200 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® XST6562 Polyester Film, 200 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Melinex® XST6562 is a thermally stabilized high clarity polyester film with good handleability. It is pretreated on one film surface to promote adhesion.Information provided by DuPont.
Physical Properties Metric English Comments
Density 1.395 g/cc
0.05040 lb/in³
ASTM D1505
Water Vapor Transmission 14.0 g/m²/day

@Temperature 38.0 °C
0.900 g/100 in²/day

@Temperature 100 °F
90% RH; ASTM F1249
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 103 MPa
15000 psi
ASTM D882A
Film Tensile Strength at Yield, TD 103 MPa
15000 psi
ASTM D882A
Film Elongation at Break, MD 160 %
160 %
ASTM D882A
Film Elongation at Break, TD 90 %
90 %
ASTM D882A
Film Tensile Strength at Break, MD 179 MPa
26000 psi
ASTM D882A
Film Tensile Strength at Break, TD 221 MPa
32000 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 0.10 %

@Temperature 150 °C,
Time 1800 sec
0.10 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 0.00 %

@Temperature 150 °C,
Time 1800 sec
0.00 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Optical Properties Metric English Comments
Optical Density 0.50
0.50
ASTM D1003
Electrical Properties Metric English Comments
Dielectric Strength 197 kV/mm
5000 kV/in
1/4" electrode 500 V/sec 25°C in air; ASTM D149
Dielectric Breakdown 10000 V
10000 V
1/4" electrode 500 V/sec 25°C in air; ASTM D149
Users viewing this material also viewed the following: