Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Teijin Films Melinex® SWC Polyester Film, 500 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® SWC Polyester Film, 500 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provided by DuPont.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 103 MPa
15000 psi
ASTM D882A
Film Tensile Strength at Yield, TD 103 MPa
15000 psi
ASTM D882A
Film Elongation at Break, MD 150 %
150 %
ASTM D882A
Film Elongation at Break, TD 120 %
120 %
ASTM D882A
Coefficient of Friction, Dynamic 0.40
0.40
A-B; ASTM D1894
Film Tensile Strength at Break, MD 193 MPa
28000 psi
ASTM D882A
Film Tensile Strength at Break, TD 221 MPa
32000 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 3.0 %

@Temperature 190 °C,
Time 300 sec
3.0 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 1.0 %

@Temperature 190 °C,
Time 300 sec
1.0 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Transmission, Visible 85.7 %
85.7 %
TLT; ASTM D1003
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm

@Temperature 25.0 °C
1.00e+17 ohm-cm

@Temperature 77.0 °F
100 V DC 50% RH 1000 sec electrification time; ASTM D257
Surface Resistivity per Square 1.00e+15 ohm

@Temperature 25.0 °C
1.00e+15 ohm

@Temperature 77.0 °F
500 V DC @ 50% RH; ASTM D257
Dielectric Strength 118 kV/mm
3000 kV/in
1/4" electrode 500 V/sec 25°C in air; ASTM D149
Dielectric Breakdown 15000 V
15000 V
1/4" electrode 500 V/sec 25°C in air; ASTM D149
Dissipation Factor 0.0030

@Frequency 100 Hz,
Temperature 25.0 °C
0.0030

@Frequency 100 Hz,
Temperature 77.0 °F
ASTM D150
0.0056

@Frequency 1000 Hz,
Temperature 25.0 °C
0.0056

@Frequency 1000 Hz,
Temperature 77.0 °F
ASTM D150