Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 90.0 g | 0.198 lb | F<sub>50</sub>; ASTM D1709/A |
NOVA Chemicals Novapol® LA-0219-A LDPE Foam Resin Features: Good heat sealing latitudeModerate toughnessEasy processability Applications: Industrial packagingLinersBlends with LLDPEFoam ArticlesInformation provided by Nova Chemicals |
|||
Dart Drop Test | 90.0 g | 0.198 lb | F50; ASTM D 1709/A |
NOVA Chemicals Surpass® FPs225-A Octene Copolymer sLLDPE Film Resin FPs225-A complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without .. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | F50; ISO 7765-1 |
Polimeri Europa Clearflex® CM 406 Hexene Copolymer Linear Low Density Polyethylene Clearflex CM 406 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.Films manufactured with Clearflex CM 406 are characterized by h.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | 25µ; ISO 7765-1 |
Total Finathene® LL 4010 FE 18 LLDPE film
(discontinued **) Linear low density polyethylene made by gas phase process for blown film applications. Advised temperature profile: 190 to 220°C.Information provided provided by Total Petrochemicals.Total Petroche.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709 |
Huntsman Rexell® M3104 Blown Film Extrusion LLDPE
(discontinued **) Linear-low medium density copolymer, cast film extrusion, FDA compliant.Features: Excellent combination of toughness, stiffness, and optics with good temperature resistance.Applications: Diaper film.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709 |
ExxonMobil LD 146.NH Cast Film Resin
(discontinued **) LD 146.NH is a homopolymer film resin offering good clarity, toughness, and stiffness. It is used in food packaging and laminating film.Information provided by ExxonMobil Chemical |
|||
Dart Drop Test | 90.0 - 100 g | 0.198 - 0.221 lb | ASTM D1709 |
Huntsman PE 1008 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Superior strength, good machinability, and heat seal characteristics.Applications: Film extrusion: industrial packaging, frozen food, produce bags, shrink, a.. |
|||
Dart Drop Test | 90.0 - 105 g | 0.198 - 0.232 lb | ASTM D1709 |
Huntsman PE 1011 Film Extrusion Polyethylene
(discontinued **) Homopolymer, Drug Master File listed product, and FDA compliant.Features: Good impact strength, good machinability, heat seal and foaming characteristicsApplications: Film Extrusion: industrial line.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709 |
Huntsman PE1033 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Good opticals, impact strength, good processing properties, and stiffnessApplications: Film extrusion: general purpose packaging and film applications.FDA No.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709A |
LyondellBasell Montell 16502F3 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, no slip, no antiblockApplications: can liners and trash bags, blends, thin filmsMeets FDA.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA345009 Low Density Polyethylene (Film Extrusion) ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA345013 Low Density Polyethylene (Film Extrusion) ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA345184 Low Density Polyethylene (Film Extrusion) ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709 |
Iran Petrochemical (PCC) LL0220KJ Linear Low Density Polyethylene LL0220KJ are linear low density polyethylene copolymers containing butane-1 as the comonomer.Applications: shipping sacks, carrier and garbage bags, consumer packaging, high clarity film, agricultu.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709 |
SCG Chemicals EL-Leneâ„¢ L2020F Linear Low Density Polyethylene Film Key Characteristics:High output and elongationContains 1800 ppm slip agent and 1400 ppm antiblocking agentRecommended Applications:General purpose bag, cast film, small bag, merchandise bag, printed.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709 |
Westlake EF4060 Low Density Polyethylene Westlake Polyethylene EF4060 is a low density formulation suggested for cast film applications that require good clarity and heat sealability. Common applications include bread bags, fresh produce b.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709A |
ExxonMobil Escorene™ LD 723.28 Cast Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra UL 723.28 is a high VA extrusion coating resin, which provides outstanding heat sealability and high clarity. LD 723.28 has a good balance of drawabilty and neck-.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709 |
ExxonMobil LD 124.MS General Purpose Clarity Film Resin Product Description: LD 124.MS blown film resin offers an excellent balance of optical and strength properties for general purpose clear film applications. Availability: Latin America, North America.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709A |
ExxonMobil LLDPE LL 3003.32 Linear Low Density Polyethylene Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709A |
ExxonMobil LLDPE LL 3003.39 Linear Low Density Polyethylene Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM-D1709 |
Braskem F7018 LDPE Injection Molding Polyethylene F7018 is a low-density polyethylene with excellent processability and sealability at low temperatures. It does not contain additives. Its applications include: extrusion coating, injection molding .. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM-D1709 |
Braskem FM31D LLDPE Blown Film Extrusion Polyethylene Copolymer The FM31D resin is a linear low-density polyethylene, copolymer of butene-1, produced by the solution process for blown film extrusion. It has excellent mechanical properties, especially hot tack. I.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM-D1709 |
Braskem LL318 LLDPE Linear Low Density Extrusion Polyethylene LL318 is a linear low-density polyethylene, copolymer of butene-1, produced by the Spherilene process. It was developed for cast film extrusion. Films obtained with this product show good mechanical.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM-D1709 |
Braskem LL6901S LLDPE Blown Film Extrusion Polyethylene Copolymer LL6901S is a LLDPE Butene copolymer produced by Braskem. It is a ready to use product since it's been compounded with 15% LDPE. It is a general purpose product that shows a good processing performan.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D-1709A |
Bapolene® 122B Polyethylene, Film Grade Bapolene LL122B is a general purpose LLDPE for blown film extrusion. This resin offers excellent tensile and toughness properties. Contains no slip and no antiblock additives. This product meets .. |
|||
Dart Drop Test | 90.0 - 126 g | 0.198 - 0.278 lb | Average value: 106 g Grade Count:6 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709 |
ExxonMobil Exceed™ 3527PA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 3527PA is a metallocene ethylene-hexene copolymer. Films made of Exceed 3527PA have high modulus and outstanding tensile, impact and puncture resistance properties. These.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709 |
Huntsman PE1158 EVA Film Extrusion
(discontinued **) 1.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LL-3002 LLDPE/Hexene Premium Cast Stretch Film Resin, 0.8 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3002 have outstanding tensile properties as well as stiffness and toughness. These su.. |