Braskem FM31D LLDPE Blown Film Extrusion Polyethylene Copolymer

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE)/Butene, Film
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Braskem FM31D LLDPE Blown Film Extrusion Polyethylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
The FM31D resin is a linear low-density polyethylene, copolymer of butene-1, produced by the solution process for blown film extrusion. It has excellent mechanical properties, especially hot tack. It contains processing aid, antiblock, slip, and antioxidant additives. Its applications include: general purpose pure and blends; and laminating and automatic packaging of solids and liquids. The FM31D resin can be processed with polyethylene on conventional extruders with a maximum ratio of 30%. The best results are of low melt index. The recommended temperature profile for blends with LDPE is slightly higher than those ones for the conventional LDPE (10 to 20ºC). Recommended blow up ratio: 1.8 to 3.0:1.
Physical Properties Metric English Comments
Density 0.919 g/cc
0.0332 lb/in³
ASTM-D792
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 860 %
860 %
ASTM-D882
Film Elongation at Break, TD 1140 %
1140 %
ASTM-D882
Elmendorf Tear Strength MD 100 g
100 g
ASTM-D1922
Elmendorf Tear Strength TD 380 g
380 g
ASTM-D1922
Elmendorf Tear Strength, MD 4.00 g/micron
102 g/mil
ASTM-D1922
Elmendorf Tear Strength, TD 15.2 g/micron
386 g/mil
ASTM-D1922
Dart Drop 3.60 g/micron
91.4 g/mil
ASTM-D1709
Dart Drop Test 90.0 g
0.198 lb
ASTM-D1709
Film Tensile Strength at Break, MD 30.0 MPa
4350 psi
ASTM-D882
Film Tensile Strength at Break, TD 20.0 MPa
2900 psi
ASTM-D882
1% Secant Modulus, MD 150 MPa
21800 psi
ASTM-D882
1% Secant Modulus, TD 170 MPa
24700 psi
ASTM-D882
Optical Properties Metric English Comments
Haze 21 %
21 %
ASTM-D1003
Gloss 76 %
76 %
Angle 60°; ASTM-D2457