Mechanical Properties Metric English Comments
Dart Drop Test >= 850 g
>= 1.87 lb
Method B; ASTM D1709
Dow AFFINITY™ PF 1140G Polyolefin Plastomer (POP)
AFFINITY™ PF 1140G is an ethylene alpha-olefin resin produced via INSITE™ Technologies. It is designed to be used in a variety of demanding applications including form-fill-seal packaging and fre..
Dart Drop Test >= 850 g
>= 1.87 lb
Method B; ASTM D1709
Dow ATTANE™ 4404G, 0.8mil Ultra Low Density Ethylene/Octene Copolymer
ATTANE™ 4201G provides improved cling in one-sided cling applications, and has improved toughness and optical properties. It complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a.Information provided by..
Dart Drop Test >= 850 g
>= 1.87 lb
Method B; ASTM D1709
Dow ATTANE™ 4404G, 2mil Ultra Low Density Ethylene/Octene Copolymer
ATTANE™ 4201G provides improved cling in one-sided cling applications, and has improved toughness and optical properties. It complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a.Information provided by..
Dart Drop Test >= 850 g
>= 1.87 lb
Method B; ASTM D1709
Dow ELITE™ 5400G Enhanced Polyethylene Resin
™ 5400G is a copolymer produced via INSITE™ Technology from Dow Plastics. It offers a unique combination of low seal initiation, moderate stiffness and low blocking tendencies for good performanc..
Dart Drop Test >= 850 g
>= 1.87 lb
Method B; ASTM D1709
Dow ELITE™ 5401G Enhanced Polyethylene Resin
™ 5401G is a copolymer produced via INSITE™ Technology from Dow Plastics. It offers a unique combination of low seal initiation, moderate stiffness and low blocking for excellent performance on a..
Dart Drop Test >= 850 g
>= 1.87 lb
gF/50%f; ASTM D1709
Braskem Flexus® 9200 Blown Film Extrusion Polyethylene
Description: Flexus 9200 is a LLDPE hexene copolymer produced through metallocene catalyst which presents excellent impact and puncture strength, beyond a differential sealing performance comparing ..
Dart Drop Test >= 850 g
>= 1.87 lb
ASTM-D1709
Braskem Flexus® 9211 LLDPE Blow Film Extrusion Polyethylene Copolymer
Braskem Flexus 9211 is a LLDPE hexene copolymer produced through a metallocene catalyst, which presents excellent impact and puncture strength beyond a differential sealing performance compared with..
Dart Drop Test >= 850 g
>= 1.87 lb
ASTM D1709
M. Holland Company MAGMA® LM203-C LLDPE  (discontinued **)
Features: Good Heat Seal, Good Tear Strength, Good ToughnessUses: BlendingProcessing Method: ExtrusionInformation provided by M. Holland.
Dart Drop Test >= 850 g
>= 1.87 lb
ASTM D1709
M. Holland Company MAGMA® LM213-C LLDPE  (discontinued **)
Features: Good Heat Seal, Good Tear Strength, Good ToughnessUses: BlendingProcessing Method: ExtrusionInformation provided by M. Holland.