Polymer Property : Dart Drop Test = 70.0 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop Test 70.0 g
0.154 lb
F50; ISO 7765-1
Polimeri Europa Clearflex® H&T FHH 508 Octene Copolymer Linear Medium Density Polyethylene
Clearflex H&T FHH 508 is an octene copolymer linear medium density polyethylene (C8-LMDPE), with antioxidant, suitable for blown film extrusion.Films obtained from Clearflex H&T FHH 508 show good op..
Dart Drop Test 70.0 g
0.154 lb
F50; ISO 7765-1
Polimeri Europa Eraclene® FC 82 High Density Polyethylene - Blown Film Extrusion
Eraclene FC 82 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Its broad molecular weight distribution and density successfully co..
Dart Drop Test >= 70.0 g
>= 0.154 lb
ASTM D1709
NIZHNEKAMSKNEFTEKHIM PE 4118Q (18403) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Dart Drop Test 70.0 g
0.154 lb
F50; ASTM D-1709
ExxonMobil Escorene® LL-1117 LLDPE Film/Sandwich Bag Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.An LLDPE blown film resin. Films made from LL-1117 have very good tensile properties and toughness. This resin's good strength and drawability all..
Dart Drop Test 70.0 g
0.154 lb
ASTM D1709
ExxonMobil LD 145.PX Packaging Resin  (discontinued **)
LD 145.PX resin is a homopolymer cast film resin offering good clarity and toughness. Applications include Bread bags and other Food Packaging.Information provided by ExxonMobil Chemical
Dart Drop Test 70.0 g
0.154 lb
F50; ASTM D-1709
ExxonMobil Escorene® LD-104 LDPE Packaging Film Resin, High Clarity  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer packaging film resin with excellent clarity and good stiffness. It is excellent either blown film or chill roll casting equipment. I..
Dart Drop Test 70.0 - 700 g
0.154 - 1.54 lb
Average value: 270 g Grade Count:96
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a..
Dart Drop Test 70.0 g
0.154 lb
F50; ASTM D-1709
ExxonMobil Escorene® LD-708 EVA Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 15.5% vinyl acetate copolymer film resin. Film made from LD-708 exhibits good impact strength and superior heat sealability.Applications: Primal ..
Dart Drop Test 70.0 g
0.154 lb
ASTM D1709
Iran Petrochemical (PCC) 235F7 Linear Low Density Polyethylene
235F7 is a LLDPE blown film grade designed for general purpose film application. This resin is particularly suited for blending with LDPE, giving better strength and downgauging possibility.Informat..
Dart Drop Test 70.0 g

@Thickness 0.0250 mm
0.154 lb

@Thickness 0.000984 in
ISO 7765-1
Borealis FG5199 Linear Low Density Polyethylene
FG5199 is a Butene Linear Low Density Polyethylene for Film Extrusion. Includes antioxidant, anti-Fog and cling additives. The grade is developed for blown cling film. Film made from FG5199 is suit..
Dart Drop Test 70.0 g
0.154 lb
ASTM D1709
ExxonMobil LD 129.24 Cast Overwrap Film Resin
Product Description: LD 129.24 is a medium density homopolymer film resin with good clarity and excellent stiffness. Film made from LD 129.24 can be used in overwrap applications and in push-through..
Dart Drop Test 70.0 g
0.154 lb
ASTM D1709A
ExxonMobil LDPE LD 104BR Low Density Polyethylene Resin
Product Description: LD 104BR is an LDPE grade, which offers good optical properties combined with increased stiffness.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antibloc..
Dart Drop Test 70.0 g
0.154 lb
ASTM D1709A
ExxonMobil LDPE LD 129.24 Low Density Polyethylene Resin
Product Description: LD 129.24 is a medium density homopolymer film resin with good clarity and excellent stiffness. Film made from LD 129.24 can be used in overwrap applications and in push-through..
Dart Drop Test 70.0 g
0.154 lb
ASTM D1709A
ExxonMobil LDPE LD 160AT Low Density Polyethylene Resin
Product Description: LD 160 series are LDPE grades, which offer good draw down and optical properties.Availability: Africa & Middle East, Asia Pacific, Latin America, North America and South America..
Dart Drop Test 70.0 g
0.154 lb
ASTM D1709A
ExxonMobil LDPE LD 380BA Blown Low Density Polyethylene Resin (European Grade)
Product Description: LD 380BA offers good toughness and optical properties.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: NoApplications: Coextrus..
Dart Drop Test 70.0 g
0.154 lb
ASTM D1709A
ExxonMobil LLDPE LL 1002.09 Linear Low Density Polyethylene Resin
Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat..
Dart Drop Test 70.0 g
0.154 lb
ASTM D1709A
ExxonMobil LLDPE LL 1002.80 Linear Low Density Polyethylene Resin
Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat..
Dart Drop Test 70.0 g
0.154 lb
ASTM D1709A
ExxonMobil LLDPE LL 1002X75 Linear Low Density Polyethylene Resin
Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat..
Dart Drop Test 70.0 g
0.154 lb
ASTM D1709A
ExxonMobil LLDPE LL 1201KG Linear Low Density Polyethylene Resin (European Grade)
Product Description: LL 1201 series are LLDPE grades, offering excellent combination of stiffness and optical properties (when blended with 10-20% LDPE) Availability: Africa & Middle East, Asia Paci..
Dart Drop Test 70.0 g
0.154 lb
ASTM D1709A
ExxonMobil LLDPE LL 1201XV Linear Low Density Polyethylene Resin (European Grade)
Product Description: LL 1201 series are LLDPE grades, offering excellent combination of stiffness and optical properties (when blended with 10-20% LDPE) Availability: Africa & Middle East, Asia Paci..
Dart Drop Test 70.0 g
0.154 lb
gF/50%f; ASTM D1709
Braskem EB853/72 Blown Film Extrusion Low Density Polyethylene
Automatic packaging for several products; High transparency films.Additives: Antiblock, DInformation provided by Braskem.
Dart Drop Test 70.0 g
0.154 lb
g/F50; ASTM D1709
Braskem F2022/0 Cast Film Extrusion Low Density Polyethylene
Films for diapers and absorbent articles; Medium resistance films or for general use.Information provided by Braskem.
Dart Drop Test 70.0 g
0.154 lb
ASTM-D1709
Braskem F2022/0 LDPE Cast Film Extrusion Polyethylene
LDPE F2022/0 has excellent sealing characteristics and optical properties with well balanced mechanical properties. Its applications include: general purpose which require no additives; shrink film..
Dart Drop Test 70.0 - 290 g
0.154 - 0.639 lb
Average value: 138 g Grade Count:14
Overview of materials for Linear Low Density Polyethylene (LLDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Blow Molding Grade". Each property range of values reported is ..
Dart Drop Test 70.0 - 850 g
0.154 - 1.87 lb
Average value: 226 g Grade Count:41
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade". Each property range of values reported is m..
Dart Drop Test 70.0 g
0.154 lb
F50; ASTM D-1709
ExxonMobil Escorene® LL-3218 LLDPE/Hexene Premium Cast Stretch Film Resin, 0.8 mil  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3218 have outstanding tensile properties as well as stiffness and toughness. These su..