Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem F2022/0 LDPE Cast Film Extrusion Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem F2022/0 LDPE Cast Film Extrusion Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LDPE F2022/0 has excellent sealing characteristics and optical properties with well balanced mechanical properties. Its applications include: general purpose which require no additives; shrink films for goods; flat film for diapers; and injection blow molding. Recommended film thickness: 0.025-0.100mm.
Physical Properties Metric English Comments
Density 0.922 g/cc
0.0333 lb/in³
ASTM-D792
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 230 %
230 %
ASTM-D882
Film Elongation at Break, TD 900 %
900 %
ASTM-D882
Elmendorf Tear Strength TD 90 g
90 g
ASTM-D1922
Elmendorf Tear Strength, TD 3.60 g/micron
91.4 g/mil
ASTM-D1922
Dart Drop 2.80 g/micron
71.1 g/mil
ASTM-D1709
Dart Drop Test 70.0 g
0.154 lb
ASTM-D1709
Film Tensile Strength at Break, MD 40.0 MPa
5800 psi
ASTM-D882
Film Tensile Strength at Break, TD 20.0 MPa
2900 psi
ASTM-D882
Optical Properties Metric English Comments
Haze 8.0 %
8.0 %
ASTM-D1003
Gloss 93 %
93 %
Angle 60°; ASTM-D2457
Processing Properties Metric English Comments
Blow-up Ratio (BUR) 1.8 - 3.0
1.8 - 3.0
Blow Film Extrusion
Descriptive Properties Value Comments
Temperature Profile (°C) 120-170
Blow Film Extrusion
180-310
Blow Molding