Braskem F2022/0 Cast Film Extrusion Low Density Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer Braskem
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem F2022/0 Cast Film Extrusion Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Films for diapers and absorbent articles; Medium resistance films or for general use.Information provided by Braskem.
Physical Properties Metric English Comments
Specific Gravity 0.922 g/cc
0.922 g/cc
ASTM D1505/D792
Thickness 25.0 microns
0.984 mil
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 230 %
230 %
ASTM D882
Film Elongation at Break, TD 900 %
900 %
ASTM D882
Elmendorf Tear Strength TD 90 g
90 g
gF; ASTM D1922
Dart Drop Test 70.0 g
0.154 lb
g/F50; ASTM D1709
Film Tensile Strength at Break, MD 40.0 MPa
5800 psi
ASTM D882
Film Tensile Strength at Break, TD 20.0 MPa
2900 psi
ASTM D882
Optical Properties Metric English Comments
Haze 8.0 %

@Thickness 0.0250 mm
8.0 %

@Thickness 0.000984 in
ASTM D1003
Gloss 93 %

@Thickness 0.0250 mm
93 %

@Thickness 0.000984 in
60°; ASTM D2457