| Category | Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade |
| Manufacturer | |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | ExxonMobil LD 145.PX Packaging Resin
(discontinued **).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.921 g/cc | 0.0333 lb/in³ | ExxonMobil Method |
| Thickness | 38.1 microns | 1.50 mil | |
| Melt Flow | 3.0 g/10 min | 3.0 g/10 min | ExxonMobil Method |
| Antiblock Level | 6000 ppm | 6000 ppm | |
| Slip Level | 1600 ppm | 1600 ppm |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Film Tensile Strength at Yield, MD | 8.00 MPa | 1160 psi | at 2% offset; ASTM D882 |
| Film Tensile Strength at Yield, TD | 7.38 MPa | 1070 psi | at 2% offset; ASTM D882 |
| Film Elongation at Break, MD | 180 % | 180 % | ASTM D882 |
| Film Elongation at Break, TD | 540 % | 540 % | ASTM D882 |
| Film Elongation at Yield, MD | 7.1 % | 7.1 % | ASTM D882 |
| Film Elongation at Yield, TD | 5.8 % | 5.8 % | ASTM D882 |
| Elmendorf Tear Strength MD | 280 g | 280 g | ASTM D1922 |
| Elmendorf Tear Strength TD | 180 g | 180 g | ASTM D1922 |
| Elmendorf Tear Strength, MD | 7.346 g/micron | 186.6 g/mil | ASTM D1922 |
| Elmendorf Tear Strength, TD | 4.72 g/micron | 120 g/mil | ASTM D1922 |
| Dart Drop | 1.83 g/micron | 46.6 g/mil | ASTM D1709 |
| Dart Drop Test | 70.0 g | 0.154 lb | ASTM D1709 |
| Film Tensile Strength at Break, MD | 22.9 MPa | 3320 psi | ASTM D882 |
| Film Tensile Strength at Break, TD | 13.5 MPa | 1960 psi | ASTM D882 |
| 1% Secant Modulus, MD | 152 MPa | 22000 psi | ASTM D882 |
| 1% Secant Modulus, TD | 163 MPa | 23600 psi | ASTM D882 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 109 °C | 228 °F | Peak Melting Temperature; ExxonMobil Method |
| Crystallization Temperature | 96.0 °C | 205 °F | ExxonMobil Method |
| Vicat Softening Point | 93.3 °C | 200 °F | ASTM D1525 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Haze | 7.0 % | 7.0 % | ASTM D1003 |
| Gloss | 72 % | 72 % | 45°; ASTM D2457 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Features | Thermal Stabilizer |