Polymer Property : Film Tensile Strength at Yield, TD = 4350 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 30.0 MPa
4350 psi
ASTM D882
SABIC F01552 High Density Polyethylene for Blown Film
Product Description: F01552 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh..
Film Tensile Strength at Yield, TD >= 30.0 MPa
>= 4350 psi
ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 4116P (16402) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Film Tensile Strength at Yield, TD >= 30.0 MPa
>= 4350 psi
ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 4121N (22401) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Film Tensile Strength at Yield, TD >= 30.0 MPa
>= 4350 psi
ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 5117P (18602) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Film Tensile Strength at Yield, TD >= 30.0 MPa
>= 4350 psi
ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 5118P (18602) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Film Tensile Strength at Yield, TD >= 30.0 MPa
>= 4350 psi
ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 5118Q (18603) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Film Tensile Strength at Yield, TD 30.0 MPa
4350 psi
ISO 527
Premix Thermoplastics PRE-ELEC® ESD 1100  (discontinued **)
PRE-ELEC ESD 1100 is a static dissipative thermoplastic compound based on PETG. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 1100 has been developed for the e..
Film Tensile Strength at Yield, TD >= 30.0 MPa
>= 4350 psi
ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 4115P (16402) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Film Tensile Strength at Yield, TD >= 30.0 MPa
>= 4350 psi
ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 4122N (22401) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Film Tensile Strength at Yield, TD 30.0 MPa
4350 psi
ASTM D882
Braskem HM 150 HDPE Monofilament Polyethylene  (discontinued **)
Applications: Raschel; flat yarn; general and industrial rape netting. Information provided by Braskem
Film Tensile Strength at Yield, TD 30.0 MPa
4350 psi
ASTM D882
Honeywell Aegisâ„¢ H100MP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H100MP is a lubricated and nucleated medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 ..
Film Tensile Strength at Yield, TD 30.0 MPa
4350 psi
ASTM D882
Honeywell Aegisâ„¢ H135MP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H135MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR..
Film Tensile Strength at Yield, TD 30.0 MPa
4350 psi
ASTM D882
Honeywell Aegisâ„¢ H135ZP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H135ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon..
Film Tensile Strength at Yield, TD 30.0 MPa
4350 psi
ASTM D882
Honeywell Aegisâ„¢ H155MP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H155MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR..
Film Tensile Strength at Yield, TD 30.0 MPa
4350 psi
ASTM D882
Honeywell Aegisâ„¢ H155ZP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H155ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well a..
Film Tensile Strength at Yield, TD 30.0 MPa
4350 psi
ASTM D882
Honeywell Aegisâ„¢ H73ZP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H73ZP is a low viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well as E..
Film Tensile Strength at Yield, TD 30.0 MPa
4350 psi
ASTM D882
SCG Chemicals EL-Leneâ„¢ H5615F High Density Polyethylene Film
Key Characteristics:High speed processingHigh tensile strengthHigh dart impactLow gel contentGood moisture barrierRecommended Applications: Ultra thin film (
Film Tensile Strength at Yield, TD 30.0 MPa
4350 psi
ISO 527-3
EMS-Grivory Grivory® CR 9 HV PA*
Product description: Grilon CR 9 HV is a high viscosity copolyamide with low temperature. Grilon CR9 HV has the following features:High flexibility and toughnessGood thermoforming and orientation pr..
Film Tensile Strength at Yield, TD 30.0 MPa
4350 psi
ISO 527-3
EMS-Grivory Grivory® CR 9 PA*
Product description: Grilon CR 9 is a copolyamide with low melting temperature. Grilon CR 9 shows the following features: High flexibility and toughnessGood thermoforming and orientation propertiesH..
Film Tensile Strength at Yield, TD 30.0 MPa
4350 psi
ISO 527-3
EMS-Grivory Grivory® F 47 H NL nat 6020 PA6
Product description: Grilon F 47 HNL natural 6020 is a nucleated, high viscosity polyamide 6. This product exhibits the following features: Good mechanical propertiesGood barrier against oils and fa..
Film Tensile Strength at Yield, TD 30.0 MPa
4350 psi
ISO 527-3
EMS-Grivory Grivory® F 40 NL PA6
Product description: Grilon F 40 NL natural 6018 is a nucleated and lubricated high viscosity polyamide 6. This product exhibits the following features: Good gas barrierGood mechanical propertiesGoo..
Film Tensile Strength at Yield, TD 30.0 MPa
4350 psi
ISO 527-3
EMS-Grivory Grivory® F 47 NL nat 6028 PA6
Product description: Grilon F 47 NL natural 6028 is a nucleated, high viscosity polyamide 6. This product exhibits the following features: Good gas barrierGood mechanical propertiesGood barrier agai..
Film Tensile Strength at Yield, TD 30.0 MPa
4350 psi
ASTM-D882
Braskem GM9450F HDPE Blown Film Extrusion Polyethylene
HDPE GM9450F is a high-density polyethylene developed for the high molecular weight film extrusion segment produced with bimodal technology. The film produced from this resin has high tenacity and e..
Film Tensile Strength at Yield, TD 30.0 MPa
4350 psi
ISO 527-3
Total XSene® HD55110 High Density Polyethylene - Blown Film
HDPE HD55110 is a bimodal high density polyethylene with a particular molecular design developed with Total Petrochemicals Double Loop Technology™.HDPE HD55110 has been especially designed for appl..
Film Tensile Strength at Yield, TD 30.0 MPa
4350 psi
Average value: 30.0 MPa Grade Count:6
Overview of materials for Nylon 6, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Film Tensile Strength at Yield, TD 30.0 MPa
4350 psi
ASTM D882
ExxonMobil Escorene® HD-7835 MMW-HDPE Blown Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A medium molecular weight HDPE blown film resin. Films made from the HD-7835 exhibit an excellent stiffness balance. HD-7835 is particularly recom..
Film Tensile Strength at Yield, TD 30.0 MPa
4350 psi
ISO 527-3
EMS-Grivory Grivory® F 50 nat 6368 PA6
Product description: Grilon F 50 natural 6368 is a modified, very high viscous Polyamide 6 for extrusion processes: Very high melt strengthGood chemical resistanceGood gas-barrierGood mechanical pro..