Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

EMS-Grivory Grivory® F 47 H NL nat 6020 PA6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® F 47 H NL nat 6020 PA6.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product description: Grilon F 47 HNL natural 6020 is a nucleated, high viscosity polyamide 6. This product exhibits the following features: Good mechanical propertiesGood barrier against oils and fatsGood heat thermal stability Application examples: Grilon F 47 HNL natural 6020 is suitable for the production of tubes and profiles. Grilon F 47 HNL natural 6020 is used as mandrel.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Water Absorption 9.0 %
9.0 %
ISO 62
Moisture Absorption 3.00 %
3.00 %
ISO 62
Water Vapor Transmission 15.0 g/m²/day
0.966 g/100 in²/day
23°C/85%r.h.; DIS 15106-1/-2
Oxygen Transmission Rate 25.0 cc/m²/day
1.61 cc/100 in²/day
23°C/0%r.h.; DIS 15105-1/-2
50.0 cc/m²/day
3.22 cc/100 in²/day
23°C/85%r.h.; DIS 15105-1/-2
Carbon Dioxide Transmission 80.0 cc-mm/m²-24hr-atm
203 cc-mil/100 in²-24hr-atm
23°C/0%r.h.; DIS 15105-1/-2
250 cc-mm/m²-24hr-atm
635 cc-mil/100 in²-24hr-atm
23°C/85%r.h.; DIS 15105-1/-2
Melt Flow 15 g/10 min
15 g/10 min
(MVR) [cm³/10min]; ISO 1133
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 35.0 MPa
5080 psi
ISO 527-3
Film Tensile Strength at Yield, TD 30.0 MPa
4350 psi
ISO 527-3
Film Elongation at Break, MD 700 %
700 %
ISO 527-3
Film Elongation at Break, TD 700 %
700 %
ISO 527-3
Film Elongation at Yield, MD 15 %
15 %
ISO 527-3
Film Elongation at Yield, TD 15 %
15 %
ISO 527-3
Tensile Modulus 0.750 GPa
109 ksi
conditioned; ISO 527-1/-2
3.00 GPa
435 ksi
dry; ISO 527-1/-2
Coefficient of Friction, Dynamic 0.25
0.25
ISO 8295
Tear Strength 30.0 kN/m
171 pli
Trouser Tear resistance MD; ISO 6383-1
30.0 kN/m
171 pli
Trouser Tear resistance TD; ISO 6383-1
Elmendorf Tear Strength MD 1020 g
1020 g
ISO 6383-2
Elmendorf Tear Strength TD 1020 g
1020 g
ISO 6383-2
Film Tensile Strength at Break, MD 100 MPa
14500 psi
ISO 527-3
Film Tensile Strength at Break, TD 90.0 MPa
13100 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
10°C/min; ISO 11357-1/-3
Optical Properties Metric English Comments
Gloss 100 %
100 %
60°; ISO 2813
Descriptive Properties Value Comments
Automotive Automotive electr. and electronics, lighting
Electricals & Electronics Cables & Tubes
Form Granules
Gelboflextest [holes/m²], EMS 900
Processing Other Extrusion
Product Attributes Barrier Properties
High viscosity
Nucleated
Special Characteristics Improved heat resistance
Users viewing this material also viewed the following: