Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.80 GPa | 696 ksi | STN EN ISO 527-2 |
Plastcom SLOVASTER® B GF 10 Polybutylene Terephthalate, 10% Glass Fiber FeaturesPBT for injection moulding, chemically reinforced with 10% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a.. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | 50 mm/min; ASTM D638 |
Ovation Polymers Opnyl OP6GF15 Nylon 6, 15% Glass Reinforced, Dry Nylon 6 - Glass reinforced (15 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. For Nylon compounds the m.. |
|||
Tensile Modulus | 4.80 GPa @Temperature 23.0 °C |
696 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
PolyOne Bergamid™ A70 G15 HW TM-Z Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Tensile Modulus | 4.80 GPa @Temperature 23.0 °C |
696 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
PolyOne Bergamid™ A70 GK30 black 13539126 Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | ASTM D638 |
Idemitsu Kosan Xarec® N WA 7010 SPS, 10% Glass Filled
(discontinued **) Crystalline Polymer Blend, Glass Filled. Used in Automotive Electronics applications. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | ISO 527 |
Nilit FRIANYL A63 KV35 Nylon 6.6 for injection molding, 35% glass ball reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | MD; ISO 527 |
Victrex® APTIV® 1102-050M Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, 20% Mineral Filled APTIV PEEK 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance application.. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | ASTM D638 |
PolyOne Stat-Tech™ AS-15GF/000 SD ABS - 15% Glass Fiber Reinforced - Antistatic Protection
(discontinued **)& Data provided by PolyOne. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | |
LATI Latilub 66-10T G/10 PA66, 10% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyamide 66 (PA66). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | |
LATI Latimass 82-03 D080 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RZL36 PA 66 (Europe-Africa-Middle East) LNP* LUBRICOMP* RZL36 is a compound based on PA 66 resin containing Milled Glass, PTFE. Added features include: Internally Lubricated. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® 1760E PBT+PC 11% Glass Reinforced alloy. Impact/chemical resistant. Excellent physical property retention in automotive exteriors. High flow version of Xenoy 1760 resin. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON PX08024 PA 6 (Europe-Africa-Middle East) LNP* STAT-KON* PX08024 is a compound based on PA 6 resin containing Mineral. Added features include; Electrically Conductive, Easy Molding. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DF0029P PC LNP THERMOCOMP* DF0029P is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Exceptional Processing. Flame Retardant. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DX07350 PC (Asia Pacific) Lexan *DX07350 resin is a glass filled, Non-brominated & Non-chlorinated flame retardant polycarbonate. High stiffness and good flow. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | 1mm/min; ISO 527-2 |
Borealis GB205U Polypropylene Compound, Glass Fiber Reinforced GB205U is a 20% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Thi.. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | ISO 527 |
Polyram RamLloy PFS302G14 ASA/PBT Alloy, 14% Glass Fiber 14% Glass fiber reinforced ASA/PBT alloy for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | ASTM-D790 |
Polyram RamOfin PPH300G4 Polypropylene, 20% Glass Fiber 20% glass fiber reinforced polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | ISO 527-1/-2 |
Covestro Bayblend® FR 3021 Polycarbonate + ABS, Mineral Filled 15 % mineral filledinjection molding gradeincreased stiffnesstensile modulus = 4800 MPaVicat/B 120 temperature = 98 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame ret.. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | ISO 527-1/-2 |
DSM Akulon® K224-HGM35 (Cond.) 15% Glass Reinforced, 25% Mineral Reinforced, Heat Stabilized Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 GX 350 HWCP Combination Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSM-30/4 PA666-MD30 Information provided by EMS Grivory |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 577 BK000 Acetal (POM)
(Unverified Data**) 20% Glass Filled Medium Viscosity Acetal Homopolymer Delrin 577 BK000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler with high stiffness low warpage and low creep for sup.. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide ALY430A PA66, Glass Fiber Reinforced, Injection Molding Staramide ALY430A is a Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Minlon® 73M30 NC010 Nylon 6
(Unverified Data**) 30% Mineral Reinforced Polyamide 6 Minlon 73M30 NC010 is a 30% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro.. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | ISO 527/4 |
Azdel Plus C321B02N 32% Chopped Fiber Mat / PP Resin Matrix AZDEL® C321B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® A3 GF 10 (2852) PA 6.6 Dry, 10% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Tensile Modulus | 4.80 GPa | 696 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics SABIC STAMAX 20YM240 PP SABIC® STAMAX 20YM240 is a 20% long glass fiber reinforced polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMDS is 62455287. |