Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.70 GPa | 537 ksi | |
Plastcom SLOVASTER® B1 GF 6/2 PBT reinforced with 6% glass fibre Features: PBT for injection moulding, chemically reinforced with 6 % glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bendi.. |
|||
Tensile Modulus | 3.70 GPa @Temperature 23.0 °C |
537 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
PolyOne Bergamid™ B700 Mi10 UF Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire PEEK is produced to the highest industry standards and is characterized by a dist.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-880 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 NL is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire PEEK is produced to the highest industry standar.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD4271 PC (Asia Pacific) Lexan* HFD4271 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4271 has enhanced mold release, impact ductility.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ISO 527 |
Aardvark Polymers Aarlon® 2000 Rotational Molding Resin, DAM Aarlon® 2000 PA 6/6 is a high performance nylon for rotational molding applications. Aarlon® 2000 offers high heat capabilities with exceptional mechanical properties.Information provided by G.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1 mm/min; ISO 527-1,-2 |
Ineos ABS Lustran® SAN C Injection Molding Grade |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | |
LATI Laticonther 83 CP/80 PA12, Impact Modified High thermal conductivity product based on Polyamide 12 (PA12), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ISO 527 |
Solvay Technyl® B 50H1 Nylon 66/6, Flame Retardant, EH0 Flame retardant copolyamide 66/6, unreinforced, heat stabilized, for injection molding.This phosphorus and halogen free flame retardant grade, UL 94 VO (0.4 mm), offers excellent filling qualities a.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ISO 527 |
Solvay Technyl® C50H2 Nylon 6, Flame Retardant, Heat Stabilized Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK) KetaSpire® KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire® PEEK is produced to the highest industry standards and is characterized b.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-880FP Polyetheretherketone (PEEK) KetaSpire® KT-880FP is the high-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural color fine powder form for compression molding and other uses that can benefit from th.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP DZ004 PC (Asia Pacific) LNP* Thermocomp* DZ004 is a compound based on Polycarbonate resin containing Glass Fiber. Also known as Thermocomp DF-1004 M |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ASTM Test |
Styrolution Luran® 358 N SAN Luran 358 N is an easy-flowing injection molding SAN grade.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ISO 527 |
Styrolution Luran® HD 20 SAN Luran HD 20 is an easy-flow grade of SAN especially designed for the medical market. It is suitable for moldings with very thin walls and / or adverse flow length to wall ratio. It features very goo.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP KFB41 (Europe-Africa-Middle East) LNP* THERMOCOMP* KFB41 is a compound based on Acetal Copolymer resin containing Glass Fiber, Glass Bead. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1mm/min; ISO 527 |
Teijin Panlite® G-3410R Glass Fiber Reinforced Polycarbonate Resin GF 10% reinforced and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecision machinery components th.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp RB003 PA 66 (Europe-Africa-Middle East) 15% glass beads filled polyamide 66 injection moulding resinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ISO 527-2 |
Styron TYRILâ„¢ 875 SAN Resin Overview: TYRIL Styrene-actylonitrile (SAN) resins are designed by Styron to offer superior chemical resistance, strength, hardness and dimensional stability in a broad range of product applications.. |
|||
Tensile Modulus | 3.70 GPa @Temperature 23.0 °C |
537 ksi @Temperature 73.4 °F |
|
Hexcel® HexPly® 954-6 Curing Cyanate Resin HexPly® 954-6 is a 250°F (121°C) curing toughened cyanate resin with 300°F (149°C) Tg. HexPly® 954-6 is formulated for autoclave curing. Recommended cure is three hours at 250°F (121°C). Ser.. |
|||
Tensile Modulus | 3.70 GPa @Temperature 23.0 °C |
537 ksi @Temperature 73.4 °F |
EN ISO 527 |
Ensinger TECASINT™ 2011 Polyimide (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 79G13HSL NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 79G13HSL is a 13% glass fiber reinforced heat stabilized lubricated slightly toughened polyamide 66 for injection molding. It has im.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide AS3 PA66, 15% Glass Bead Reinforced, Injection Molding Staramide AS3 is a 15% Glass Bead Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ISO 527 |
Cossa Polimeri ESTABLEND PA 2516 GF ABS / Nylon 6 Blend, 8% Glass Filled ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.8% glass fiber reinforcedExceptional chemical resistance, excellent heat resistance, good dimensional stabilityInformation .. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® A3 GF 15 (2418) PA 6.6 Conditioned, 15% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1mm/min; ISO 527 |
BASF Ultramid® 8202C HS PA6 (Dry) Ultramid 8202C HS is a heat stabilized, low viscosity, PA6 injection molding homopolymer possessing a modified crystalline structure for increased property performance and faster cycles. It is also.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 79G13HSL BK039 Nylon 66
(Unverified Data**) 13% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 79G13HSL BK039 is a 13 % glass reinforced heat stabilized lubricated slightly toughened black polyamide 66 for injection molding. It.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ISO 527 |
Victrex® HT™ G45 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, low flow, FDA food contact complia.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD4471 PC (Asia Pacific) Lexan* HFD4471 is a 10% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4417 has enhanced mold release, impact ductili.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD4471 PC (Europe-Africa-Middle East) Lexan* HFD4471 is a 10% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4417 has enhanced mold release, impact ductili.. |