Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.20 GPa | 319 ksi | ASTM D638 |
NCMT NanoPAC™ S201 High Performance Polypropylene Nanocomposite Characteristics: High stiffness Supplementary of ABS Good impact resistant Less shrinkage Good thermal conductivity Applications: Electrical Appliances AutomobileInformation provided by Nano Composi.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | ASTM D882 |
SABIC Innovative Plastics Lexan® FR66 Polycarbonate Film, Flame Retardant Lexan FR66 flame-retardant film is a clear, thin-gauge polycarbonate film with a suede finish on one side and a matte finish on the other, and a UL94 V-0 listing to meet the stringent requirements i.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® ML7652 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Medium flow, excellent low temperature ductility.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® BDT6500 ABS AUTOMOTIVE. Low gloss, color concentratable for interior applications. Natural only. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | ASTM D882 |
SABIC Innovative Plastics Lexan® FR63 Polycarbonate Film, Flame Retardant Lexan FR63 flame-retardant film is a clear, thin-gauge polycarbonate film with a matte finish on one side and a polish finish on the other and a UL94 V-0 listing to meet the stringent requirements i.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXD9810 PC Copolymer (Europe-Africa-Middle East) Non-chlorinated, non-brominated Flame retardant PC-siloxane copolymer blend. Excellent processability, super high flow, good impact, UL rated V-0. Limited translucent colors.This data was supplied b.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min; ISO 527 |
LG Chemical LG-749 ABS, Low Gloss, High Heat Resistance Information Provided by LG Chem |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | |
Ineos ABS Lustran® LGA Key Features:UnfilledSuitable processing methods:Injection molding |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DL003EU PC LNP LUBRICOMP* DL003EU is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Easy Molding, UV Stabilized, Internally Lubricated. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP KP004A Acetal Homopolymer LNP* LUBRICOMP* KP004A is a compound based on Acetal Homopolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 50H1 PA66, Conditioned Description: Flame retardant polyamide 66, unreinforced, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This phospho.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® SR-0330M ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOTUF R1000I PA 66 (Asia Pacific) High Impact Nylon 66 compound containing Impact Modifier. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® V3900WX PBT+PC PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | DIN 53457 |
Zell-Metall Engineering Plastics Zellamid 1200 G Zellamid® 1200 G is manufactured by an activated anionic reaction. Finished and semi-finished parts are produced by a static cast process. This process makes it possible to produce a material wit.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 GS 30 HWCP 30% Glass Sphere Filled Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | |
Covestro Bayblend® KL 1-1430 Polycarbonate/ABS Blend Standard grade for cars.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min |
Arkema Group Rilsan® AESN G9 T6L Nylon 12, Graphite Filled (Conditioned) Designation ISO 1874-PA12,EHLS,22-010,CD10Rigid grade with graphite fillers for extrusion. Available color: steel gray. Reinforced light and heat stabilizing agents.Very low friction coefficient. No.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0336W20L Wollastonite Reinforced |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0339C40L Calcium Reinforced |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | |
BASF Luranyl® KR 2420 Polyphenylene Ether + Styrene-Butadiene Blend Grade with high resistance to heat deformation and outstanding impact strength. For auto parts such as air vents or the instrument panel; also used for door-mirror housings.Data was collected by IS.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | ISO 527-2 |
CENTROPLAST CENTRODAL GL Polyoxymethylene + PE-UHMW CENTRODAL GL has good dry running and emergency running properties. During the modification of POM + PE, a PE-UHMW is incorporated to the basic polyoxymethylene polymer. It leads to an improvement.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | ISO 527-1/-2 |
Covestro Makroblend® DP UT6007 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendimpact modifiedeasy releaseUV-stabilizedinjection molding grade Makroblend DP UT6007* offers an exceptional low-temperature impact strength, good flowability and.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min |
Polimeri Europa EDISTIR PD RK6223N High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,083-12-07-23 Halogen and Antimony free, medium impact polystyrene. This grade complies at 2 mm with IEC 65-20-2 and BSI.. |