Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.30 GPa | 189 ksi | STN EN ISO 527-2 |
Plastcom SLOVALEN PC 78 FRD 1 Polypropylene Copolymer, Halogen Flame Retardant, UV Stabilized FeaturesModified copolymer PP with the possibility of changing the MFI within the interval 5 - 20 g/10min. Stabilized against the UV-radiation by the UV stabilizer on the HALS basis. Retarded with.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527 |
Quadrant EPP Cestilene™ HD 500 R Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527-1/-2 |
Quadrant EPP PE 500 PE-HMW, virgin (ISO Data) This grade exhibits a good combination of stiffness, toughness, mechanical damping ability with wear- and abrasion resistance and can easily be welded. In less demanding applications with respect to.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | DIN 53457 |
Isoflon PP Polypropylene Products with excellent friction, anti-stick, abrasion and chemical inertia characteristicsVery good impact resistanceNo moisture regainProduct for the food industryInformation provided by Isoflon. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | d.a.m.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® BC 600 HTS DUSXBL 900116 Nylon 6, Impact Modified PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® A 30 000000 Nylon 66 PA 66, standard injection molding grade, non-reinforced, very easy release, normal solidificationApplication Examples: terminal blocks, cable clips, bobbins, gearwheels |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 402 Natural FA PA66, Conditioned Description: Unreinforced polyamide PA66, very high viscosity, for extrusion.Available in: Europe and North AmericaProduct Applications: TECHNYL® A 402 NATURAL FA offers three main advantages: hi.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Stat-kon TE002 LNP* Stat-kon* TE002 is a compound based on Polyurethane resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the A.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | 1mm/min; ISO 527-2 |
Borealis BB125MO Polypropylene Copolymer BB125MO is a heterophasic copolymer. This grade is a low melt flow rate grade intended for blow molding and sheet extrusion, and features extremely good process ability with improved melt strength a.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | 1mm/min; ISO 527-2 |
Borealis BF330MO Polypropylene Copolymer BF330MO is a heterophasic copolymer. This polymer is characterized by an optimum combination of high stiffness, high impact strength and good flow properties. This grade is designed for high-speed i.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | 1mm/min; ISO 527-2 |
Borealis BJ100HP Polypropylene Copolymer BJ100HP is a special low viscosity polypropylene compound developed to fit the production of PP-GF composites in the direct LFT compression and injection molding process as well as in combination wi.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | 1mm/min; ISO 527-2 |
Borealis BJ380MO Polypropylene Copolymer BJ380MO is a very high melt flow heterophasic copolymer with high/medium impact strength and stiffness. This grade is designed for high-speed injection molding and contains nucleating and antistatic.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | 1mm/min; ISO 527-2 |
Borealis BS2581 High Density Polyethylene for Blow Molding BS2581 is a high density polyethylene intended for blow molding products with high stiffness and very good environmental stress crack resistance (ESCR). Applications: industrial chemicals, househol.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 572-2 |
Total Lumicene® MR30MC2 Metallocene Random Copolymer Polypropylene, Injection Molding Lumicene® MR30MC2 is a metallocene random copolymer with a melt flow index of 30 g/10 min for injection molding. Lumicene® MR30MC2 differs from the other random copolymers by its molding reproduci.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527-2 |
Total PPC 7612 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 7612 is a nucleated and controlled-rheology heterophasic copolymer. PPC 7612 is characterized by a good balance between rigidity and impact resistance and has excellent antistatic.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527-2 |
Total PPH 9099 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9099 is a very narrow molecular weight distribution homopolymer polypropylene, with anti gas-fading stabilization. ApplicationATOFINA Polypropylene PPH 9099 is intended for.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 572-2 |
Total PPR 7220 Random Copolymer Polypropylene, Injection Molding Total Petrochemicals PPR 7220 is a nucleated random copolymer polypropylene with a melt flow index of 10 g/10 min for the injection molding of articles with high transparency and excellent surface a.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 572-2 |
Total PPR 7227 Random Copolymer Polypropylene, Injection Molding Total Petrochemicals PPR 7227 is a high transparency random copolymer polypropylene specially developed for the injection molding of caps and closures and articles with high transparency, excellent .. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527-1, 2 |
Polyplastics Duracon® SF-20 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527-2 |
Total PPC 4663 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 4663 is heterophasic copolymer. PPC 4663 is characterized by a combination of ease of processing and good manufacturing article properties in applications ranging from hou.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 HWUVCP Nylon 66, UV Stabilized, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | Foaming Direction |
Cymat A35620SC 040SS Stabilized Aluminum Foam Description: Cymat A35620SC 040SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.4 g/cm3. The mechanical properties of SAF make it .. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4188 black 9992 PA612 Product description: Grilamid XE 4188 black 9992 is a high viscosity, unreinforced, impact resistant polyamide 612 (PA612) extrusion grade. Unique features of Grilamid XE 4188 black 9992 are: High v.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | DIN 53 457 |
Hippe PP Polypropylene Lower density compared with PE. Higher hardness and stiffness and better reset features. Non-fragile. Toughness in cold lesser than that of PE. Higher working temperatures than PE, not aromatic-.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | 1mm/min; ISO 527 |
BASF Ultraform N 2640 Z6 UNC POM Ultraform N 2640 Z6 UNC is an elastomer-modified injection molding POM grade with excellent impact strength. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527-2 |
CENTROPLAST CENTROLEN PPS Polypropylene flame resistant This material is a low density, easily machined plastic that can be welded and is flame resistant. Applications include exhaust systems for heating systems, and apparatus engineering.Information pr.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | 50 mm/min (2.0 in/min) |
Aardvark Polymers Aardalloy® 3326 POM Alloy Rotational Molding Resin Aardalloy 3326 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3326 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | Conditioned; ISO 527 Type 1 A |
Solvay Technyl® A 402 H1 Nylon 66 Unreinforced, very high viscosity, heat stabilized, for extrusion and injection molding. TECHNYL® A 402 H1 offers three main advantages: high impact resistance at low humidity levels, good rigidit.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | 1mm/min; ASTM D638 |
3M Dyneon™ PVDF 60512/0000 Polyvinylidene Fluoride
(discontinued **) Polyvinylidenefluoride (PVDF) is ideal for multiple applications across a wide array of industries. Widely used in the chemical process industry, wire and cable industry, semiconductor industry, and.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BR 40 W PA6 Product description: Grilon BR 40 W is a medium viscosity, plasticized PA6 extrusion grade. Grilon BR 40 W has the following important properties: High flexibilityHigh stiffness Grilon BR 40 W is us.. |