Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.12 g/cc | 0.0405 lb/in³ | ISO 1183 |
Water Absorption | 8.0 % | 8.0 % | ISO 62 |
Moisture Absorption | 2.50 % | 2.50 % | ISO 62 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 30.0 MPa | 4350 psi | conditioned; ISO 2039-1 |
55.0 MPa | 7980 psi | dry; ISO 2039-1 | |
Tensile Strength, Yield | 30.0 MPa | 4350 psi | dry; ISO 527-1/-2 |
40.0 MPa | 5800 psi | dry; ISO 527-1/-2 | |
Elongation at Break | >= 50 % | >= 50 % | conditioned; ISO 527-1/-2 |
<= 50 % | <= 50 % | dry; ISO 527-1/-2 | |
Elongation at Yield | 35 % | 35 % | dry; ISO 527-1/-2 |
40 % | 40 % | conditioned; ISO 527-1/-2 | |
Tensile Modulus | 0.500 GPa | 72.5 ksi | conditioned; ISO 527-1/-2 |
1.30 GPa | 189 ksi | dry; ISO 527-1/-2 | |
Charpy Impact Unnotched | NB | NB | dry; ISO 179/1eU |
NB | NB | conditioned; ISO 179/1eU | |
NB @Temperature 30.0 °C |
NB @Temperature 86.0 °F |
dry; ISO 179/1eU | |
NB @Temperature 30.0 °C |
NB @Temperature 86.0 °F |
conditioned; ISO 179/1eU | |
Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | dry; ISO 179/1eA |
NB | NB | conditioned; ISO 179/1eA | |
0.300 J/cm² @Temperature 30.0 °C |
1.43 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU | |
0.300 J/cm² @Temperature 30.0 °C |
1.43 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-1/-2 |
CTE, linear, Transverse to Flow | 160 µm/m-°C | 88.9 µin/in-°F | ISO 11359-1/-2 |
Melting Point | 220 °C | 428 °F | 10°C/min; ISO 11357-1/-3 |
Maximum Service Temperature, Air | 70.0 - 90.0 °C | 158 - 194 °F | long term; EMS |
160 °C | 320 °F | short term; EMS | |
Deflection Temperature at 0.46 MPa (66 psi) | 110 °C | 230 °F | ISO 75-1/-2 |
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 °C | 113 °F | ISO 75-1/-2 |
Flammability, UL94 | HB | HB | IEC 60695-11-10 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | conditioned; IEC 60093 |
1.00e+13 ohm-cm | 1.00e+13 ohm-cm | dry; IEC 60093 | |
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
Dielectric Strength | 22.0 kV/mm | 559 kV/in | conditioned; IEC 60243-1 |
26.0 kV/mm | 660 kV/in | dry; IEC 60243-1 | |
Comparative Tracking Index | 450 V | 450 V | conditioned; IEC 60112 |
Descriptive Properties | Value | Comments |
---|---|---|
Additives | Plasticizer | |
Automotive | Air intake sytems | |
Fuel systems | ||
Hydraulic systems | ||
Electricals & Electronics | Cables & Tubes | |
Form | Granules | |
Industry & Consumer goods | Hydraulics & Pneumatics | |
Mechanical Engineering | ||
Power transmission | ||
Tools & Accessories | ||
Processing | Injection Molding | |
Other Extrusion | ||
Product Attributes | High viscosity |