Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.10 GPa @Temperature 23.0 °C |
160 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
PolyOne Bergamid™ B70 red RAL3001 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | |
LyondellBasell Lupolen® 5236 HX HDPE, Impact Grade Medium flow, impact resistant, high stress-crack resistant grade for closures for bottles that contain carbonated liquids. This product contains a slip agent.Data was collected by ISO methods and o.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® B 30 S FN40 000000 Nylon 6 PA 6, injection molding grade, non- reinforced, good flowability, easy-release, fast cycling, UL 94V-2 off 0,75 mm, GWIT 775°C bei 0,75/1,5mm |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® B 31 SK 000000 Nylon 6 PA 6, injection molding grade, non-reinforced, easy flow, easy-release, rapid solidification, crystallizes somewhat more finely and uniformly than B 30 S |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | ISO 527 Type 1A |
Solvay TECHNYL® C 206 PA6, Conditioned Description: Unreinforced Polyamide PA6, standard for fast cycling, for injection molding.Available in: EuropeProduct Applications: TECHNYL® C 206 has fluidity and a good mould release, favored b.. |
|||
Tensile Modulus | 1.10 - 1.35 GPa @Thickness 1.50 mm |
160 - 196 ksi @Thickness 0.0591 in |
1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 60512/0550 and 60512/0150 Polyvinylidene Fluoride (PVDF) Solef® 60512/0550 and Solef® 60512/0150 are PVDF grades compounded with PTFE for extrusion of anti-wear tapes.Features: CopolymerUses: TapeAdditional Properties: Crystallization Heat - ASTM D3.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP TH0600A PUR LNP THERMOCOMP* TH0600A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | 1mm/min; ISO 527-2 |
Borealis BL0521 High Density Polyethylene BL0521 is a high molecular weight (HMW), high density polyethylene. The main properties are: good impact resistance, high stiffness, very good stress crack resistance. Applications: cans and drums .. |
|||
Tensile Modulus | 1.10 - 1.30 GPa | 160 - 189 ksi | MD; ISO 527-3 |
Borealis BorPURE™ RB501BF Polypropylene Copolymer BorPure™ RB501BF is a random copolymer. Applications: BorPure™ RB501BF has been developed especially for applications like: food packaging, over wrap film, label film, and shrink film. Additives.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | At 1 mm/min; ISO 527-2 |
Borealis Borstar® HE3494-LS Dark Blue High Density Polyethylene for Drinking Water Pipes Borstar HE3494-LS is a yellow-orange, cadmium free, high density polyethylene compound classified as a MRS 10.0 material (PE100) produced with the advanced Borstar technology. It includes a combina.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | 1mm/min; ISO 527-3 |
Borealis BorSafe™ HE3490-LS-H HDPE Compound for Pressure Pipes BorSafe™ HE3490-LS-H is a bimodal polyethylene compound produced by the advanced Borstar® technology. It includes a combination of pigments and stabilizers to ensure excellent long-term thermal s.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | 1mm/min; ISO 527-2 |
Borealis BS2541 High Density Polyethylene BS2541 is a high density polyethylene with very high ESCR This product is intended for blow molding. Applications: household and chemical containers such as detergents, cleaners, and motor oils, an.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | ISO 527-2 |
Total PPC 4660 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 4660 is heterophasic copolymer. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | |
Covestro Bayflex® 110-50 Polyurethane Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 16 LM PA12 Product Description: Grilamid L 16 LM is a , low viscosity extrusion type, based on Polyamide 12 (PA12). Grilamid L 16 LM is UV- and heat stabilized. The modification with a nucleation agent results.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 16 nat PA12 Low viscosity unmodified polyamide 12Information provided by EMS Grivory |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 20 G PA12 Product Description: Grilamid L 20 LG is a normal viscosity, heat stabilized polyamide 12 non-reinforced injection molding grade. This product has very good flow characteristics Low moisture absorpt.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 20 L PA12 Product Description: Grilamid L 20 L is a medium viscosity Polyamide 12 (PA12) extrusion type. It is UV and heat stabilized. Its main features are: High surface quality Very good UV and heat resista.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 20H FWA black 9225 PA12 Product Description Grilamid L 20 H FWA black 9225 is a medium viscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 20 H FWA black 9225 is used for technical injection molded .. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 25H FWA nat PA12 Product Description: Grilamid L 25 H FWA natural is a highviscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 25 H FWA natural is designed for technical injection moulded com.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | Foaming Direction |
Cymat A35620SC 030SS Stabilized Aluminum Foam Description: Cymat A35620SC 030SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.3 g/cm3. The mechanical properties of SAF make it .. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 3926 black 9992 PA12 Product description: Grilamid XE 3926 black 9992 is a low viscosity extrusion type, based on Polyamide 12 (PA 12). The special features of Grilamid XE 3926 black 9992 are: Very good chemical resista.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® FG408L NC010 Nylon 66
(Unverified Data**) Unreinforced Toughened Polyamide 66 with Developed for Food Contact Applications Zytel FG408L NC010 is a general purpose lubricated impact modified polyamide 66 resin with superior toughness for inj.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 CP Nylon 6, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | cond.; ISO 527 |
Azoty Tarnow™ Tarnamid® T-29 MCS Polyamide 6 - Colored Colored medium-high viscosity grade for injection molding.Tarnamid® has the following main properties:High mechanical strength, rigidity and hardnessHigh impact strengthHigh vibration damping capac.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 25 nat PA12 Product Description: Grilamid L 25 is a high viscosity polyamide 12. This product has the following features: Very tasteless High toughness, even at low temperatures Good resistance to weathering Go.. |
|||
Tensile Modulus | 1.10 GPa @Temperature 150 °C |
160 ksi @Temperature 302 °F |
ISO 527-2 |
Solvay Specialty Polymers Amodel® A-1240 L Polyphthalamide (PPA)
(discontinued **) Amodel A-1240 L is a 40% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon MD000IU PP (Asia Pacific) LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa.. |