Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.01 g/cc | 0.0365 lb/in³ | ISO 1183 |
Water Absorption | 1.5 % | 1.5 % | ISO 62 |
Moisture Absorption | 0.700 % | 0.700 % | ISO 62 |
Linear Mold Shrinkage, Flow | 0.0080 cm/cm | 0.0080 in/in | ISO 294-4, 2577 |
Linear Mold Shrinkage, Transverse | 0.0080 cm/cm | 0.0080 in/in | ISO 294-4, 2577 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore D | 70 | 70 | conditioned, 15s; ISO 868 |
Tensile Strength at Break | 50.0 MPa | 7250 psi | dry; ISO 527-1/-2 |
50.0 MPa | 7250 psi | conditioned; ISO 527-1/-2 | |
Tensile Strength, Yield | 45.0 MPa | 6530 psi | dry; ISO 527-1/-2 |
45.0 MPa | 6530 psi | dry; ISO 527-1/-2 | |
Elongation at Break | >= 50 % | >= 50 % | conditioned; ISO 527-1/-2 |
<= 50 % | <= 50 % | dry; ISO 527-1/-2 | |
Elongation at Yield | 5.0 % | 5.0 % | dry; ISO 527-1/-2 |
15 % | 15 % | conditioned; ISO 527-1/-2 | |
Tensile Modulus | 1.10 GPa | 160 ksi | conditioned; ISO 527-1/-2 |
1.50 GPa | 218 ksi | dry; ISO 527-1/-2 | |
Charpy Impact Unnotched | NB | NB | dry; ISO 179/1eU |
NB | NB | conditioned; ISO 179/1eU | |
NB @Temperature 30.0 °C |
NB @Temperature 86.0 °F |
dry; ISO 179/1eU | |
NB @Temperature 30.0 °C |
NB @Temperature 86.0 °F |
conditioned; ISO 179/1eU | |
Charpy Impact, Notched | 0.600 J/cm² | 2.86 ft-lb/in² | dry; ISO 179/1eA |
0.600 J/cm² | 2.86 ft-lb/in² | conditioned; ISO 179/1eA | |
0.600 J/cm² @Temperature 30.0 °C |
2.86 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU | |
0.700 J/cm² @Temperature 30.0 °C |
3.33 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 120 µm/m-°C | 66.7 µin/in-°F | ISO 11359-1/-2 |
CTE, linear, Transverse to Flow | 140 µm/m-°C | 77.8 µin/in-°F | ISO 11359-1/-2 |
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
Maximum Service Temperature, Air | 90.0 °C | 194 °F | long term; EMS |
150 °C | 302 °F | short term; EMS | |
Deflection Temperature at 0.46 MPa (66 psi) | 115 °C | 239 °F | ISO 75-1/-2 |
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 °C | 113 °F | ISO 75-1/-2 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | conditioned; IEC 60093 |
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
Comparative Tracking Index | 600 V | 600 V | conditioned; IEC 60112 |
Descriptive Properties | Value | Comments |
---|---|---|
Food contact | FDA | |
Form | Granules | |
Industry & Consumer goods | Housewares | |
Hydraulics & Pneumatics | ||
Mechanical Engineering | ||
Medical devices | ||
Sports & Leisure | ||
Tools & Accessories | ||
Processing | Injection Molding | |
Other Extrusion | ||
Product Attributes | Improved flowability and demoulding |