Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 10.6 GPa | 1540 ksi | d.a.m.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® AKV 30 000000 Nylon 66, Glass Fiber Reinforced PA 66, 30% glass fibers, injection moldingInformation provided by LANXESS. |
|||
Tensile Modulus | 10.6 GPa | 1540 ksi | ISO 527-1/-2 |
Lanxess Durethan® AKV 35 H2.0 901510 Nylon 66, 35% Glass Fiber PA 66, injection molding grade, 35% glass fibers, good heat-ageing resistanceApplication Examples: gearbox oil sumps, oil modules |
|||
Tensile Modulus | 10.6 GPa | 1540 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp UFL36ASP PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UFL36ASP is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE.
Added features include Internally Lubricated, Heat Stabilized.This data was supplied by SABIC-IP f.. |
|||
Tensile Modulus | 10.6 GPa | 1540 ksi | ISO 527-2 |
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire® AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This r.. |
|||
Tensile Modulus | 10.6 GPa | 1540 ksi | ASTM D638 |
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable.. |
|||
Tensile Modulus | 10.6 GPa | 1540 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DE004 PC LNP STAT-KON* DE004 is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 10.6 GPa | 1540 ksi | ISO 527-2 |
Solvay Specialty Polymers Kalix® 2930 HFFR Polyamide, High Performance (HPPA), Glass Fiber Kalix® 2930 HFFR is a bio-sourced polyamide-based material specifically formulated to meet UL 94V2 @ 0.4 mm requirements for electronic devices. The material uses an advanced halogen-free flame r.. |
|||
Tensile Modulus | 10.6 GPa | 1540 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DE004 PC (Asia Pacific) LNP STAT-KON* DE004 is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 10.6 GPa | 1540 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DEL13PXC PC (Europe-Africa-Middle East) LNP* Stat-kon* DEL13PXC is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Superior Molding. |
|||
Tensile Modulus | 10.6 GPa | 1540 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DF0079 PC (Europe-Africa-Middle East) LNP* Thermocomp* DF0079 is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant. |
|||
Tensile Modulus | 10.6 GPa | 1540 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_PCN2910 PPE+PS LNP* Thermodcomp* Noryl_PCN2910 compound is a 35% Glass/Mica filled. High modulus and tight tolerance molding for the chassis market. |
|||
Tensile Modulus | 10.6 GPa | 1540 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP QFL17RS PA 6/10 LNP LUBRICOMP* QFL17RS is a compound based on Nylon 6/10 resin containing 35% Glass Fiber, 5% PTFE. Added features of this material include: Easy Release, Heat Stabilized, Wear Resistant. |
|||
Tensile Modulus | 10.6 GPa | 1540 ksi | ASTM D638 |
Plenco 6527 Phenolic, Granular, Transfer Molded PLENCO 06527 is a woodflour and mineral filled resole phenolic molding compound.Information supplied by Plenco. |
|||
Tensile Modulus | 10.6 GPa | 1540 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Sorona® 3030GV BK001 Polytrimethylene Terephthalate (PTT) 30% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3030GV BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% based .. |
|||
Tensile Modulus | 10.6 GPa | 1540 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R533 NT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533 NT is general-purpose, 33% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade that is lubricated for good machine feed, flow and mold release. Gl.. |
|||
Tensile Modulus | 10.6 GPa | 1540 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R533H NT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H NT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties .. |
|||
Tensile Modulus | 10.6 GPa | 1540 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R533H01 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H01 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties whe.. |
|||
Tensile Modulus | 10.6 GPa | 1540 ksi | ISO 527-2/1A/1 |
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This resin ret.. |
|||
Tensile Modulus | 10.6 GPa | 1540 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R533H BK02 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK02 is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when exposed to anti-f.. |
|||
Tensile Modulus | 10.6 GPa | 1540 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R533H BK0201 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK0201 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Tensile Modulus | 10.6 GPa | 1540 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R533H BK10A0 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK10A0 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Tensile Modulus | 10.6 GPa @Temperature 23.0 °C |
1540 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Sorona® 3030G BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& Sorona® 3030G BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% polymer basis) with good strength, stiffness and low warpage and superior s.. |
|||
Tensile Modulus | 10.6 GPa @Temperature 23.0 °C |
1540 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Sorona® 3030GV BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® 3030GV BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness a.. |
|||
Tensile Modulus | 10.6 GPa | 1540 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R533 Nylon 66, 33% Glass Filled, Dry as Molded Vydyne® R533 is general-purpose, 33% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for good machine feed, flow, and mold release. Glas.. |