Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.70 GPa | 1410 ksi | |
Radici Radilon® A RV300R (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Tensile Modulus | 9.75 GPa | 1410 ksi | ISO 527-1/2 |
Radici Radilon® ARV300 (dry) Nylon 66 30% Glass-fiber reinforcedInformation provided by Radici group. |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | ISO 527-1/2 |
Radici Radilon® SRV300 (dry) Nylon 6 Glass-fiber reinforcedInformation provided by Radici group. |
|||
Tensile Modulus | 9.72 GPa | 1410 ksi | ASTM D638 |
LNP Thermocomp® LF-1006 MG Polyetheretherketone, Glass milled Glass Fiber
(discontinued **) Features: Low WarpageForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still a.. |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | 1 mm/min; ISO 527-1,-2 |
Gromax BFG30-FN00N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | ISO 527-1/-2 |
Lanxess Durethan® BKV 330 H2.0 901510 Nylon 6, 30% Glass Fiber PA 6, injection molding type, 30% glass fibers, branched/structural viscosity, good weldability (vibration or hot plate), good heat-ageing resistance |
|||
Tensile Modulus | 9.72 GPa | 1410 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP IFP36 PA6.12 LNP* LUBRICOMP* IFP36 is a Nylon 6/12 base resin containing 30% Glass Fiber, 15% PTFE/Silicone. Added features of t his grade include: Wear Resistant. |
|||
Tensile Modulus | 9.72 GPa | 1410 ksi | ISO 527 |
Solvay Technyl® C 218 MT25 V15 25% Mineral, 15% Glass Filled, Heat Stabilized Nylon 6 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36SXC PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFL36SXC is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36SXD PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFL36SXD is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
Tensile Modulus | 9.69 GPa | 1410 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 771 PBT (Europe-Africa-Middle East) VALOX 771 is a 15% glass and 20% mineral filled, flame retarded injection moulding PBT resin. |
|||
Tensile Modulus | 9.72 GPa | 1410 ksi | ASTM D638 |
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI) Torlon® 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not .. |
|||
Tensile Modulus | 9.75 GPa | 1410 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® 6370 PBT+PC 30% glass-reinforced, impact modified thermoplastic alloy. Improved toughness and ductility. |
|||
Tensile Modulus | 9.71 GPa | 1410 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP DF0069P PC LNP THERMOCOMP* DF0069P is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Exceptional Processing. Flame Retardant. |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP JX97000 PES (Europe-Africa-Middle East) LNP* Thermocomp* JX97000 is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Mold Release. |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | dry; ISO 527-1/-2 |
DSM Novamid® 3021GH30 NAT PA66-GF30 30% Glass Reinforced, Heat Stabilized |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSG-30 PA666-GF30 Product description: Grilon TSG-30 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSG-30 has the following important properties: Excellent fl.. |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSG-30/4 FA PA666-GF30 Information provided by EMS Grivory |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSG-30/4 PA666-GF30 Product description: Grilon TSG-30/4 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSG-30/4 has the following important properties: Good flo.. |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSG-30/4 W PA666-GF30 Product description: Grilon TSG-30/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | dry; DIN 53 457 |
Hippe PA 66 GF 30 Nylon 66 30% Glass fiber Reinforced These polyamide components being reinforced with glass fiber up to 30% are not only highly wear-resistant, but also show high mechanical strength, stiffness and dimensional stability. They can also.. |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | ISO 527-1/-2 |
Polyplastic Armamid® PA6 GF 30 HS-901 Nylon, 30% Glass Filled Injection molding, heat stabilizedInformation provided by PolyPlastic Group. |
|||
Tensile Modulus | 9.70 GPa | 1410 ksi | |
LATI Latigray 82-05 CX/90 PA 12 Radiopaque compound based on Polyamide 12 (PA12). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Tensile Modulus | 9.74 GPa | 1410 ksi | ISO 527-1/-2 |
Kuraray Genestar™ G1300A-M41 Nylon, 30% Glass Filled Glass reinforced injection grade. Main Features:Chemical resistanceHeat resistanceExamples of applications:Gears and bearing retainersIntercooler tank and turbo duct pipe |