Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.50 GPa | 1380 ksi | |
Plastcom SLOVASTER® B/E GF 30 PBT, 30% glass fibre FeaturesPBT/PET for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and ben.. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | ISO 527 |
Nilit FRIANYL A63 W-GV30 Nylon 6.6, std. viscosity for injection molding, 30% glass fiber reinforced Nylon 6.6, std. viscosity for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | >= 9.50 GPa | >= 1380 ksi | ISO 527-1,2 |
Qualchem Danamid AFGF-50 Polyamide 66, 50% Glass Fiber Reinforced with glass fiberInformation provided by Qualchem Zrt. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | cond.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® BKV 50 H EF DUS022 900116 Nylon 6, Glass Fiber Reinforced PA 6, 50% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | DAM; ISO 527 Type 1 A |
Solvay Technyl® A 60G1 V25 25% Glass Reinforced Nylon 66, Flame Retardant This Red Phosphorous and Halogen free flame retardant grade, combines excellent all-round mechanical properties with outstanding flame retardancy (UL 5VA at 1.6mm) and electrical performance. This p.. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 2310R PEI (Europe-Africa-Middle East) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM HU2310 PEI (Asia Pacific) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Asia Pacific) VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Tensile Modulus | 9.49 GPa | 1380 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® SHF436HR PBT (Asia Pacific) PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | dry; ISO 527-1/-2 |
DSM Akulon® K224-G6-FC 99.99.99 PA6-GF30 30% Glass Reinforced, Food Contact Grade |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | ISO 527-1/-2 |
DSM Akulon® S223-HG6 Nylon 66-30% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | ISO 527-1/-2 |
DSM Akulon® Ultraflow™ K-FG6 Nylon 6-30% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-30 S FA PA6-GF30 Product description: Grilon BG-30 S FA is a heat stabilized PA6 injection molding grade with 30% glass fibers. Grilon BG-30 S FA has the following important properties: Excellent surface finishEasy .. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-30/2 PA6-GF30 Product description: Grilon BG-30/2 is a heat stabilized, normal viscosity PA6 injection molding grade with 30% glass fibers. Grilon BG-30/2 has the following important properties: High stiffnessGoo.. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 GV 30 HWCP 30% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 GV 40 HWCP 40% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® HT XE 3996 PA*-GF30 Product description: Grivory XE 3996 black 9225 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. ISO-Polymer designatio.. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4104 nat PA610-GF40 Product description: Grilamid XE 4104 natural is a 40% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw materia.. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4107 nat PA612-GF40 Product description: Grilamid XE 4107 natural is a 40% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4107 are: low water absorptiong.. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® SC193 NC010 PBT+SAN
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Blend Developed for the Healthcare IndustryCrastin® SC193 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. It.. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam AFR460B PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR460B is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | ISO 527 |
Eurotec® Tecodur® PB70 GR30 NL100 PBT, 20% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | dry; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 GF30 TF15 Polyamide 6 - Improved Slip Properties Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Low wear and low friction grade, contains molybdenum disulfide, PTFE.Tarnamid.. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | ISO 527 |
BASF Ultramid® B3WG6 CR BK 23210 15% Glass Filled (Dry) Description: Ultramid B3WG6 CR BK23210 s a 30% glass fiber reinforced, heat stabilized injection molding PA6 grade for crash relevant applications.Information provided by BASF |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | ISO 527-1/-2 |
DSM Akulon® K224-TG9 Nylon 6-45% Glass Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® VX4930 PBT (Europe-Africa-Middle East) VALOX VX4930 is a 30% glass reinforced nucleated PBT/ASA blend with excellent mechanical properties, high dimensional stability and low density. Applications: connectors and automotive industry. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | ASTM D638 |
Solvay Specialty Polymers Ixef® 2010/X914 Polyarylamide, 40% Filler, DAM
(discontinued **) The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |