Polymer Property : Tensile Modulus = 9.49 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Modulus 9.49 GPa
1380 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Valox® SHF436HR PBT
PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant.
Tensile Modulus 9.49 GPa
1380 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Valox® SHF436HR PBT (Asia Pacific)
PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant.
Tensile Modulus 9.49 GPa
1380 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Valox® SHF436HR PBT (Europe-Africa-Middle East)
PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant.