Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 8.70 GPa | 1260 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DFP36 PC LNP* LUBRICOMP* DFP36 is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE/Silicone. Added features include: Internally Lubricated. |
|||
Tensile Modulus | 8.69 GPa | 1260 ksi | ASTM D638 |
Solvay Specialty Polymers Udel® GF-130 Polysulfone (PSU)
(Unverified Data**) Udel GF-130, resin is a 30% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resi.. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | ISO 527-1/-2 |
DSM Akulon® S223-PG6U (Dry) 33% Glass Reinforced, Impact Modified Nylon 66 (North America)
(discontinued **)& Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | ASTM D638 |
Plenco 7527 Phenolic, Nodular, Injection Molded
(discontinued **) Single-Stage Phenolic. PLENCO 07527 is a flock cotton and mineral filled resole phenolic molding compound.Information supplied by Plenco |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 21T2 V25 PA66, 25% glass fiber, DRY Description: Flame retardant polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Appl.. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RX05050 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RX05050 is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 8.72 GPa | 1260 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY DF206XXH PC LNP* LUBRILOY* DF206XXH is a compound based on Polycarbonate containing 30% Glass Fiber, Proprietary Lubricant. Added features of this grade include: Wear Resistant, Healthcare. |
|||
Tensile Modulus | 8.69 GPa | 1260 ksi | ASTM D638 |
Solvay Specialty Polymers Udel® GF-130 Polysulfone (PSU), Glass Fiber Udel® GF-130, resin is a 30% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical .. |
|||
Tensile Modulus | 8.69 GPa | 1260 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON REL42 PA 66 (Asia Pacific) LNP* Stat-kon* REL42 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON SE002Z PA 12 (Asia Pacific) LNP* Stat-kon* SE002Z is a compound based on Nylon 12 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 8.67 GPa | 1260 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp RFZ71S PA 66 LNP* Thermocomp* RFZ71S is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for t.. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218 V35 Black 34 NG PA66, 35% glass fiber, Conditioned Description: TECHNYL® A 218 V35 Black 34 NG is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Tensile Modulus | 8.68 GPa | 1260 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Stat-kon DE002P PC (Asia Pacific) LNP STAT-KON* DE002P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the .. |
|||
Tensile Modulus | 8.66 GPa | 1260 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 430 PBT 33 % glass reinforced, impact modified. Connectors, etc. |
|||
Tensile Modulus | 8.66 GPa | 1260 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 430 PBT (Asia Pacific) 33 % glass reinforced, impact modified. Connectors, etc. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermotuf PF007IX2 PA 6 (Europe-Africa-Middle East) LNP * THERMOTUF* PF007IX2 is a compound based on PA 6 resin containing Glass Fiber. Added features include: High Impact.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | ISO 527-1/-2 |
Unitika BV2120G30 PA66, 30% Glass Fiber Reinforced, Flame Retardant, Conditioned Information provided by Unitika Ltd. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | ASTM D638 |
Plenco 5482 Phenolic, Granular, Injection Molded PLENCO 05482 is an organic reinforced phenolic molding compound formulated with graphite to improve the abrasion resistance. 05482 is available in black and brown. 05482 is not recommended for elect.. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | ASTM D638 |
Plenco 5482 Phenolic, Granular, Transfer Molded PLENCO 05482 is an organic reinforced phenolic molding compound formulated with graphite to improve the abrasion resistance. 05482 is available in black and brown. 05482 is not recommended for elect.. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-30 HM PA6-GF30 Product description: Grilon BG-30 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 30% glass fibers. Grilon BG-30 HM has the following important prop.. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® FR95G25V0NH NC010 Nylon 66
(Unverified Data**) 25% Glass Reinforced Flame Retardant Polyamide 66 ZYTEL FR95G25V0NH NC010 is 25% glass fiber reinforced flame retardant polyamide halogen and red phosphorous free with high flow and excellent long t.. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide PF007IX2 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide PF007IX1 is an Impact Modified, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as Star X 2010 33V)Information provided by Eurostar. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam AFR560B5 PA66, Mineral/Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR560B5 is a Flame Retardant, Mineral Filled and Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | ISO 527-2 |
CENTROPLAST CENTROMID 6 GF 30 Polyamide 6 30% glass fiber The 30% glass fibre matrix adds very high strength and rigidity to this material. It has increased dimensional accuracy when hot. Can be used for rollers, belt pulleys and racks.Information provid.. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | |
LATI Latimass 82-03 D110 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Tensile Modulus | 8.68 GPa | 1260 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP PH0800A PA 6 LNP* THERMOCOMP* PH0800A is a compound based on Nylon 6 resin. Added feature of this material is: High Specific Gravity. |