Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Woodflour Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Plenco 5482 Phenolic, Granular, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PLENCO 05482 is an organic reinforced phenolic molding compound formulated with graphite to improve the abrasion resistance. 05482 is available in black and brown. 05482 is not recommended for electrical insulating applications.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.660 g/cc
0.0238 lb/in³
ASTM D1895
Density 1.43 g/cc
0.0517 lb/in³
ASTM D792
Water Absorption 0.30 %
0.30 %
ASTM D570
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 88
88
ASTM D785
Tensile Strength, Ultimate 64.0 MPa
9280 psi
ASTM D638
Elongation at Break 0.92 %
0.92 %
ASTM D638
Tensile Modulus 8.70 GPa
1260 ksi
ASTM D638
Flexural Strength 95.0 MPa
13800 psi
ASTM D790
Flexural Modulus 7.40 GPa
1070 ksi
ASTM D790
Compressive Strength 208 MPa
30200 psi
ASTM D695
Izod Impact, Notched 0.163 J/cm
0.305 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.184 J/cm²
0.876 ft-lb/in²
ASTM D256
Impact 99
99
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 52.0 µm/m-°C

@Temperature 40.0 - 130 °C
28.9 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.440 W/m-K

@Temperature 100 °C
3.05 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 200 °C
392 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 157 °C
315 °F
ASTM D648
Oxygen Index 28.3 %
28.3 %
ASTM D2863
Shrinkage 0.30 %
0.30 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 2.60e+11 ohm-cm
2.60e+11 ohm-cm
ASTM D247
Dielectric Constant 5.7
5.7
ASTM D150
Dielectric Strength 9.10 kV/mm
231 kV/in
Short Time; ASTM D149
Dissipation Factor 0.050
0.050
ASTM D150
Arc Resistance 25 sec
25 sec
ASTM D495
Comparative Tracking Index 200 V
200 V
ASTM D3638