Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.50 GPa @Temperature 23.0 °C |
1380 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® CE15330 BK010 PBT
(Unverified Data**) Crastin® CE15330 BK010 is a 30% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance.. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | ISO 527, ASTM D638 |
Nilit Nilamid B3 H G6 30% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G6 is a general purpose, 30% glass fiber reinforced NYLON 6 with a combination of good mechanical performance, impact strength and processability. It is one of the most wid.. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | ISO 527-1/-2 |
DSM Akulon® S223-HG6U (Dry) 33% Glass Reinforced Nylon 66 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | cond.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® BKV 50 H EF DUS022 900116 Nylon 6, Glass Fiber Reinforced PA 6, 50% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | ISO 527-1/-2 |
Lanxess Durethan® BKV 30 H2.0 901510 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, good heat-ageing resistanceApplication Examples: pedal brackets, automotive front end structures |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | d.a.m.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® DP BKV 35 XF 901510 Nylon 6, 35% Glass Fiber PA 6, 35% glass fibers, injection molding, improved flowability, improved surface finishInformation provided by LANXESS. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 2300 PEI (Europe-Africa-Middle East) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 2300F PEI 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM HU2110 PEI 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP .. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM HU2300 PEI 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP .. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM HU2310 PEI 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 771 PBT (Europe-Africa-Middle East) VALOX 771 is a 15% glass and 20% mineral filled, flame retarded injection moulding PBT resin. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp RF0069 PA 66 (Europe-Africa-Middle East) Flame retarded, 30% glass fibre reinforced Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RF006S PA6.6 (Europe-Africa-Middle East) LNP* THERMOCOMP* RF006S is a compound based on PA 66 resin containing Glass Fiber. Added features include: Heat Stabilized. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp PF006 PA 6 (Europe-Africa-Middle East) 30% glass fibre reinforced Polyamide 6 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | ISO 527-1/-2 |
DSM Akulon® K224-G6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | dry; ISO 527-1/-2 |
DSM Akulon® K224-G6-FC BK00001 PA6-GF30 30% Glass Reinforced, Food Contact Grade |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | ISO 527-1/-2 |
DSM Akulon® S223-HG6 (Dry) 30% Glass Reinforced Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | dry; ISO 527-1/-2 |
DSM EcoPaXX® Q-KG6 PA410-GF30 % Glass Reinforced, Heat Stabilized, for E&E applications |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-30/2 PA6-GF30 Product description: Grilon BG-30/2 is a heat stabilized, normal viscosity PA6 injection molding grade with 30% glass fibers. Grilon BG-30/2 has the following important properties: High stiffnessGoo.. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TSGL-40/4 nat PA666-GF40 Product description: Grilon TSGL-40/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 40% long glass fibers. Grilon TSGL-40/4 natural is characterized by the following .. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 5026 (BG-30 H) PA6-GF30 Product description: Grilon B XE 5026 (BG-30 H) black 9922 is a high heat stabilized, 30% glass fiber reinforced PA6- Injection molding grade with modified flowability. Grilon B XE 5026 (BG-30 H) bl.. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® LW9030 NC010 PBT+ASA
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. .. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide PF006 PA6, 30% Glass Fiber Filled, Injection Molded Staramide PF06 is an 30% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide PF006S PA6, 30% Glass Fiber Filled, Injection Molded Staramide PF006S is a 30% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam AFR460B PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR460B is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | ISO 527 |
Eurotec® Tecodur® PB70 GR30 NL PBT 30% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Tensile Modulus | 9.50 GPa | 1380 ksi | ASTM D638 |
Solvay Specialty Polymers Ixef® 2010/X914 Polyarylamide, 40% Filler, DAM
(discontinued **) The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |