Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 8.62 GPa | 1250 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ PS-30GF/2S Natural Polybutylene Terephthalate (PBT) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 8.62 GPa | 1250 ksi | ASTM D638 |
PolyOne Nymax™ GF 924 33 UV Black 108 Polyamide 66 (Nylon 66) Property data for molded test bars: Dry as MoldedInformation provided by PolyOne |
|||
Tensile Modulus | 8.62 GPa | 1250 ksi | ASTM D638 |
Oxford Polymers 30GF 30% Glass Fiber Filled Polycarbonate for Injection Molding 30% Glass Fiber Filled Polycarbonate for Injection MoldingInformation provided by Oxford Polymers. |
|||
Tensile Modulus | 8.62 GPa | 1250 ksi | ASTM D638 |
PolyOne Nymax™ GF 1200 A 33 HS Black 22 Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Tensile Modulus | 8.62 GPa | 1250 ksi | ASTM D638 |
Solvay Specialty Polymers Veradel® AG-230 Polyethersulfone
(discontinued **) For superior long-term performance at high temperatures in severe service environments. It offers especially good toughness, hydrolytic stability, chemical resistance, plus FDA and USDA compliance.N.. |
|||
Tensile Modulus | 8.62 GPa | 1250 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ 80530 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 8.62 GPa | 1250 ksi | ASTM D638 |
Fiberfil® J-69/40/E High performance polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 8.62 GPa | 1250 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP EX07305 PEI (Asia Pacific) Polyetherimide reinforced with Glass fiber and PTFE for use in Burn-in Test Sockets (BiTS) Application |
|||
Tensile Modulus | 8.62 GPa | 1250 ksi | ASTM D638 |
Solvay Specialty Polymers Veradel® 3330GF Polyethersulfone (PESU), 30% Glass Fiber Veradel® 3330GF is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, .. |
|||
Tensile Modulus | 8.62 GPa | 1250 ksi | ASTM D638 |
Solvay Specialty Polymers Veradel® 3430GF Polyethersulfone (PESU), 30% Glass Fiber Veradel® 3430GF is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, .. |
|||
Tensile Modulus | 8.62 GPa | 1250 ksi | ASTM D638 |
Solvay Specialty Polymers Veradel® AG-330 Polyethersulfone (PESU), 30% Glass Fiber Veradel® AG-330 is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, .. |
|||
Tensile Modulus | 8.62 GPa | 1250 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP LF004E PEEK LNP* THERMOCOMP* LF004E is a compound based on Polyetheretherketone resin containing 20% Glass Fiber. Added features of this material include: Easy Molding. |
|||
Tensile Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
Plastics Group Polifil® GFPC-30 30% Glass-Reinforced Polycarbonate Polifil® GFPC series compounds offer a combination of improved dimensional stability and decreased flammability. The excellent balance of physical properties make the Polifil® glass-filled polycar.. |
|||
Tensile Modulus | 8.62 GPa | 1250 ksi | ASTM D638 |
Solvay Specialty Polymers Veradel® 3330GF Polyethersulfone (PESU)
(Unverified Data**) Veradel 3330GF is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dime.. |