Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Veradel® 3430GF Polyethersulfone (PESU), 30% Glass Fiber

Category Polymer , Thermoplastic , Polyethersulfone (PES) , Polyethersulfone (PES), 30%Glass Fiber Filled
Manufacturer Solvay Specialty Polymers
Trade Name Veradel®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Solvay Specialty Polymers Veradel® 3430GF Polyethersulfone (PESU), 30% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Veradel® 3430GF is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resistance of the material, while maintaining most of its other basic characteristics. The combination of structural properties and cost effectiveness make this resin an attractive alternative to metals in many engineering applications.Features: Acid Resistant; Flame Retardant; Good Adhesion; Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Thermal Stability; Good Toughness; High Heat Resistance; High Rigidity; High Tensile Strength; Hydrolysis Resistant; Medium Flow; Medium Molecular WeightUses: Appliance Components; Appliances; Automotive Electronics; Batteries; Business Equipment; Electrical Parts; Electrical/Electronic Applications; Food Service Applications; Industrial Applications; Metal Replacement; Microwave Cookware; Plumbing Parts; Valves/Valve PartsInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.58 g/cc
0.0571 lb/in³
ASTM D792
Filler Content 30 %
30 %
Glass Fiber
Water Absorption 0.40 %
<br>@Time 86400 sec
0.40 %
<br>@Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
Melt Flow 4.5 g/10 min
<br>@Load 2.16 kg,<br> Temperature 343 °C
4.5 g/10 min
<br>@Load 4.76 lb,<br> Temperature 649 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 130 MPa
18900 psi
ASTM D638
Elongation at Break 1.9 %
1.9 %
ASTM D638
Tensile Modulus 8.62 GPa
1250 ksi
ASTM D638
Flexural Strength 179 MPa
26000 psi
ASTM D790
Flexural Modulus 8.62 GPa
1250 ksi
ASTM D790
Izod Impact, Notched 0.750 J/cm
1.41 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 31.0 µm/m-°C
17.2 µin/in-°F
Deflection Temperature at 1.8 MPa (264 psi) 216 °C
421 °F
Unannealed; ASTM D648
Flammability, UL94 V-0
<br>@Thickness 0.787 mm
V-0
<br>@Thickness 0.0310 in
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+16 ohm-cm
>= 1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 4.11
<br>@Frequency 60.0 Hz
4.11
<br>@Frequency 60.0 Hz
ASTM D150
4.13
<br>@Frequency 1000 Hz
4.13
<br>@Frequency 1000 Hz
ASTM D150
4.17
<br>@Frequency 1.00e+6 Hz
4.17
<br>@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm
432 kV/in
ASTM D149
Dissipation Factor 0.0018
<br>@Frequency 1000 Hz
0.0018
<br>@Frequency 1000 Hz
ASTM D150
0.0019
<br>@Frequency 60.0 Hz
0.0019
<br>@Frequency 60.0 Hz
ASTM D150
0.0094
<br>@Frequency 1.00e+6 Hz
0.0094
<br>@Frequency 1.00e+6 Hz
ASTM D150
Compliance Properties Metric English Comments
NSF Yes
Yes
NSF 61
Processing Properties Metric English Comments
Melt Temperature 343 - 399 °C
649 - 750 °F
Mold Temperature 149 - 163 °C
300 - 325 °F
Drying Temperature 149 - 177 °C
<br>@Time 9000 - 14400 sec
300 - 351 °F
<br>@Time 2.50 - 4.00 hour
Descriptive Properties Value Comments
Agency Ratings NSF 61
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Colors Available; Opaque
Form Pellets
Injection Rate Fast
Processing Technique Injection Molding
RoHS Compliance RoHS Compliant
Screw Compression Ratio 2.0:1.0
Copyright © lookpolymers.com All Rights Reserved