Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.00 GPa | 1020 ksi | same value from ASTM and ISO test. |
BASF Capron® GR20 20% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR20 is a 20% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also.. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ASTM D638 |
Gharda Chemicals Gafone™ 3610GM20 Polyethersulfone (PES)
(discontinued **) Characteristics: Excellent Thermal Resistance - Tg 224°C Outstanding Mechanical, Electrical, Flame & Chemical Resistance Very good Hydrolytic & Sterilization Resistance Good Optical Cl.. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527 |
Nilit FRIANYL A63 H-GV20 Nylon 6.6 for injection molding, 20% glass fiber reinforced Nylon 6.6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | 1 mm/min; ISO 527 - 1/2 |
Hexion Bakelite™ PF 85 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, organically filled, reinforced with cotton fibers, average notched impact strength, UL listed molding compound 1.5 mm/HB (BK, BN).Application areas: Switch covers, rolls, .. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | |
LATI Latishield 85-08A G/20 PES, Steel/Glass Fibers EMI shielding product based on Polyether Sulfone (PES). Steel fibers. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati .. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218HP V35 PA66, 35% glass fiber, Conditioned Description: TECHNYL® A 218HP V35 is a polyamide 6.6, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product of.. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 30 H1 V25 PA66, 25% glass fiber, Conditioned Description: Flame-retardant polyamide 66, 25% glass-fiber reinforced, heat stabilized for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications:.. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | DIN 53457 |
Schwartz Technical Plastics LAMINEX® 2000 Cotton Fabric, Phenolic Resin Impregnated, Coarse Application: rollneck-bearings, coverts for friction rollsInformation provided by Schwartz Technical Plastics GmbH |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | DIN 53457 |
Schwartz Technical Plastics LAMINEX® 2040 Cotton Fabric, Phenolic Resin Impregnated, MoS2 Filled Application: slippers, gear-rods, bushesInformation provided by Schwartz Technical Plastics GmbH |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® DR48V PBT (Europe-Africa-Middle East) VALOX DR48V is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot.. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON PFD04S PA 6 (Europe-Africa-Middle East) LNP* Statkon* PFD04S is a compound based on PA 6 resin containing Glass Fiber, Carbon Powder. Added features include: Electrically Conductive, Heat Stabilized. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX8720 PPE+PA (Asia Pacific) Noryl GTX* GTX8720 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-.. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GTX GTX8720 PPE+PA (Europe-Africa-Middle East) Noryl GTX* GTX8720 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-.. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527-1/-2 |
DSM Akulon® K223-HM6 (BLACK) Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | cond; ISO 527-1/-2 |
DSM EcoPaXX® Q-KG6 PA410-GF30 % Glass Reinforced, Heat Stabilized, for E&E applications |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 MRGV 20/10 HWCP 20% Mineral and 10% Glass Fiber Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® HT2V-15H PA6T/66-GF15 Product description: Grivory HT2V-15H is a 15 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO.. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN 52GM50EF WT001 Polyphthalamide (PPA)
(Unverified Data**) 50% Glass/Mineral Reinforced PPA High Performance Polyamide Zytel HTN52GM50EF WT001 is a glass and mineral reinforced high performance polyamide resin developed for LED reflector applications. It is.. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527 |
Eurotec® Tecodur® PB70 BR20 NL100 HS PBT, 20% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527 |
Eurotec® Tecopet® PT70 GR15 NL100 PR PET, 15% glass fiber reinforced, heat stabilized, natural, fast crystallization grade Information provided by Eurotec® |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | cond; ISO 527-1/-2 |
DSM EcoPaXX® Q-HG6 PA410-GF30 30% Glass Reinforced, Heat Stabilized |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527 |
Eurotec® Tecodur® PB70 GR20 NL PBT 20% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527 |
Eurotec® Tecomid® MB40 GR20 NL PA6, 20% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Tensile Modulus | 7.00 GPa @Treatment Temp. 70.0 °C, Time 576000 sec |
1020 ksi @Treatment Temp. 158 °F, Time 160 hour |
62% rel. humidity |
Akro-Plastic Akromid® S3 GF 30 1 (3222) PA 6.10 Dry, 30% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | 1 mm/min |
Arkema Group Kynar® 9000 HDC N 123 PVDF
(discontinued **) Designation ISO 12086-PVDF-E,GG1,Q.5E5.J.A.I.D, CF,Kynar PVDF are fluorinated thermoplastic homopolymers.Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, high barrier.. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527-1/-2 |
DSM Akulon® K-FKGS6 (Cond.) 30% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 7.00 GPa @Temperature 180 °C |
1020 ksi @Temperature 356 °F |
ISO 527-1/-2 |
DSM Stanyl® TS200F10 PA46-GF50 50% Glass Reinforced |