Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gharda Chemicals Gafone™ 3610GM20 Polyethersulfone (PES)  (discontinued **)

Category Polymer , Thermoplastic , Polyethersulfone (PES)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gharda Chemicals Gafone™ 3610GM20 Polyethersulfone (PES)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Characteristics: Excellent Thermal Resistance - Tg 224°C Outstanding Mechanical, Electrical, Flame & Chemical Resistance Very good Hydrolytic & Sterilization Resistance Good Optical Clarity Processed by all Conventional Techniques Applications: Clear applications like baby bottle, snuffer buttons, tee lights etc. Membrane applications Industrial and domestic coating Medical - Sterilizable box, surgical instrument Automotive - engine components Household - microwave oven food trays Industrial - oil level indicator, high temp. lighting fixture, Heat exchanger parts Electrical - Printed circuit board Information provided by Gharda ChemicalsSolvay Advanced Polymers completed its acquisition of this product line in May 2006.
Physical Properties Metric English Comments
Specific Gravity 1.62 g/cc
1.62 g/cc
ASTM D792
Filler Content 30 %
30 %
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 85.0 MPa
12300 psi
ASTM D638
Elongation at Break 2.1 %
2.1 %
ASTM D638
Tensile Modulus 7.00 GPa
1020 ksi
ASTM D638
Flexural Strength 130 MPa
18900 psi
ASTM D790
Flexural Modulus 7.00 GPa
1020 ksi
ASTM D790
Izod Impact, Notched 0.380 J/cm
0.712 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 190 °C
374 °F
Continuous Use; UL-746B
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ASTM D648
Glass Transition Temp, Tg 225 °C
437 °F
ASTM D3482
Flammability, UL94 V-0

@Thickness 0.900 mm
V-0

@Thickness 0.0354 in
UL 94
Oxygen Index 41 %
41 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+16 ohm-cm
>= 1.00e+16 ohm-cm
ASTM D257
Surface Resistance >= 1.00e+14 ohm
>= 1.00e+14 ohm
ASTM D257
Dielectric Strength 20.0 kV/mm
508 kV/in
ASTM D149
Arc Resistance 125 sec
125 sec
ASTM D495
Comparative Tracking Index 150 V
150 V
ASTM D3638
Users viewing this material also viewed the following: