Mechanical Properties Metric English Comments
Tensile Modulus 2.95 GPa
428 ksi
STN EN ISO 527-2
Plastcom PLASTALEN® PH 51 T 40 Polypropylene reinforced with mineral filler
Modified homopolymer PP for injection molding with the content of 40% mineral filler. General application. Delivered in black color.Information Provided by Plastcom spol. s r.o.
Tensile Modulus 2.95 GPa
428 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics Cycoloy® CX7010 PC+ABS
Cycoloy* CX7010 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0. Excellent flow combined with good balance of pro..
Tensile Modulus 2.95 GPa
428 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics Cycoloy® CX7010 PC+ABS (Asia Pacific)
Cycoloy* CX7010 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0. Excellent flow combined with good balance of pro..
Tensile Modulus 2.95 GPa
428 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics Cycoloy® CX7010 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX7010 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0. Excellent flow combined with good balance of pro..
Tensile Modulus 2.95 GPa
428 ksi
ASTM D638
Nilit Polynil® C50L Externally Lubricated PA66/6
Description: Polynil C50L shows better surface finish, flow and elongation than a comparable homopolymer. Key characteristics: Excellent flowHigh elongationGood impact strengthGood overall mechanica..
Tensile Modulus 2.95 GPa
428 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Cycoloy® CX7211 PC+ABS
Cycoloy* CX7211 PC/ABS resin is a non-filled, injection moldable grade which has UL 94 rating at 2.5 mm 5VA. Cycoloy CX7211 resin provides all color options and features an excellent balance of flo..
Tensile Modulus 2.95 GPa
428 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Cycoloy® CX7211 PC+ABS (Asia Pacific)
Cycoloy* CX7211 PC/ABS resin is a non-filled, injection moldable grade which has UL 94 rating at 2.5 mm 5VA. Cycoloy CX7211 resin provides all color options and features an excellent balance of flo..
Tensile Modulus 2.95 GPa
428 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS
Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc..
Tensile Modulus 2.95 GPa
428 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS (Asia Pacific)
Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc..
Tensile Modulus 2.95 GPa
428 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc..
Tensile Modulus 2.95 GPa
428 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics Cycoloy® CY5211 PC+ABS (Asia Pacific)
CY5211 is a FR PC+ABS of non-brominated, non-chlorinated flame retardant systems with balanced flow, impact and hydrolytic stability.This data was supplied by SABIC-IP for the Asia Pacific region.
Tensile Modulus 2.95 GPa
428 ksi
ISO 527-1/-2
Quadrant EPP Acetron® MD POM-C + metal detectable additive, extruded (ISO Data)
Metal detectable POM-C grade High mechanical strength, stiffness and hardness Excellent resilience Good creep resistance High impact strength, even at low temperatures Very good dimensional stabilit..
Tensile Modulus 2.95 GPa
428 ksi
Radici Radilon® A CP400 (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Tensile Modulus 2.95 GPa
428 ksi
ISO 5271/2
Radici Radilon® S 40FL (dry) Nylon 6
Radilon® S (homopolyamides) are normally used in cast and blown extrusion for the production of packaging films. Radilon® S grades can be extruded to a thickness varying from 20 mm to 100 mm.Appl..
Tensile Modulus 2.95 GPa
428 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Dry Blend E1500 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Modulus 2.95 GPa
428 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Dry Blend E1501 Polyvinyl Chloride, Rigid (PVC, Rigid)
VSI FLAMMABILITY:Burn Length (0.040 in Bar)ASTM D635 0* IN.Burn Time (0.040 in Bar) ASTM D635 0* Sec.*Extinguished before 25 MM starting ref mark.Information provided by PolyOne
Tensile Modulus 2.95 GPa
428 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Cycoloy® CX7211 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX7211 PC/ABS resin is a non-filled, injection moldable grade which has UL 94 rating at 2.5 mm 5VA. Cycoloy CX7211 resin provides all color options and features an excellent balance of flo..
Tensile Modulus 2.95 GPa
428 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP IN001 PA6.12
LNP* LUBRICOMP* IN001 is a compound based on Nylon 6/12 resin containing 2% Moly. Added feature of this grade is: Wear Resistant.
Tensile Modulus 2.95 GPa
428 ksi
ISO 527 Type 1A
Solvay TECHNYL® C 216 PA6, DRY
Description: Unreinforced polyamide PA6, standard nucleation for fast cycling, for injection molding.Available in: Asia PacificProduct Applications: This grade has a high fluidity and good mould rel..
Tensile Modulus 2.95 GPa
428 ksi
ISO 527
Solvay Technyl® C 217 Unfilled, Heat Stabilized, Impact Modified Nylon 6
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Tensile Modulus 2.95 GPa
428 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP RP004S PA 66
LNP* LUBRICOMP* RP004S is a compound based on Nylon 66 containing PTFE/Silicone. Added features of this grade include: Heat Stabilized, Wear Resistant.
Tensile Modulus 2.95 GPa
428 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL N850 PPE+PS
ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical and Business Equipment applications.
Tensile Modulus 2.95 GPa
428 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL N850 PPE+PS (Asia Pacific)
ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical and Business Equipment applications.
Tensile Modulus 2.95 GPa
428 ksi
ISO 527 Type 1A
Solvay TECHNYL® A 32G1 PA66, DRY
Description: Flame retardant Polyamide 66, unreinforced, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: This flame r..
Tensile Modulus 2.95 GPa
428 ksi
DIN 53457/ISO 527
Wico Plast Wicotal 500 Acetal
ApplicationsInjection moldingAll information provided by Wico Plast, Warenhandelsges. mbH
Tensile Modulus 2.95 GPa
428 ksi
DIN 53457/ISO 527
Wico Plast Wicotal 90 Acetal
ApplicationsInjection moldingAll information provided by Wico Plast, Warenhandelsges. mbH
Tensile Modulus 2.95 GPa
428 ksi
Secant; ISO 527-2/50
ExxonMobil Exxtral™ CMN 303 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin designed for high heat ageing resistance for automotive interior trim applications such as instrument panels.Availability: Africa & Mi..
Tensile Modulus 2.95 GPa
428 ksi
ISO 527-1/-2
DuPont Performance Polymers Delrin® 100P NC010 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer with Improved Processing Delrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. It has improved processing thermal stability good mechani..
Tensile Modulus 2.95 GPa
428 ksi
1mm/min; ISO 527-2