Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wico Plast Wicotal 90 Acetal

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced
Manufacturer Wico Plast
Trade Name Wicotal
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wico Plast Wicotal 90 Acetal.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
ApplicationsInjection moldingAll information provided by Wico Plast, Warenhandelsges. mbH
Physical Properties Metric English Comments
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 64.0 MPa
9280 psi
DIN 53455/ISO 527
Tensile Modulus 2.95 GPa
428 ksi
DIN 53457/ISO 527
Izod Impact, Unnotched (ISO) NB
NB
DIN 53453