Quadrant EPP Acetron® MD POM-C + metal detectable additive, extruded (ISO Data)

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced
Manufacturer Quadrant Engineering Plastics Products
Trade Name Acetron®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Acetron® MD POM-C + metal detectable additive, extruded (ISO Data).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Metal detectable POM-C grade High mechanical strength, stiffness and hardness Excellent resilience Good creep resistance High impact strength, even at low temperatures Very good dimensional stability (low water absorption) Good sliding properties and wear resistance Excellent machinability Good electrical insulating and dielectric properties Physiologically inert (most grades are suitable for food contact) Not self-extinguishing Food contact compliant according to FDA, and EU Directive 2002/72 EC Continuous use temperature up to 105 °C (221 °F) Metal and visual detection by blue color; metal detection level for particles 3mm x 3mm x 3mm Detection by x-ray also possible
Physical Properties Metric English Comments
Density 1.46 g/cc
0.0527 lb/in³
ISO 1183-1
Moisture Absorption at Equilibrium 0.19 %
0.19 %
50% RH
Water Absorption at Saturation 0.75 %
0.75 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 86
86
ISO 2039-2
Hardness, Shore D 80
80
Ball Indentation Hardness 155 MPa
22500 psi
ISO 2039-1
Tensile Strength 66.0 MPa
9570 psi
at Yield; ISO 527-1/-2
Elongation at Break 15 %
15 %
ISO 527-1/-2
Elongation at Yield 14 %
14 %
ISO 527-1/-2
Tensile Modulus 2.95 GPa
428 ksi
ISO 527-1/-2
Flexural Strength 93.0 MPa
13500 psi
Flexural Modulus 2.80 GPa
406 ksi
Compressive Strength 25.0 MPa

@Strain 1 %
3630 psi

@Strain 1 %
ISO 604
44.0 MPa

@Strain 2 %
6380 psi

@Strain 2 %
ISO 604
76.0 MPa

@Strain 5 %
11000 psi

@Strain 5 %
ISO 604
K Factor (ISO) 45 µm/km
45 µm/km
Charpy Impact Unnotched 7.00 J/cm²
33.3 ft-lb/in²
ISO 179-1/1eU
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.30 - 0.45
0.30 - 0.45
Thermal Properties Metric English Comments
CTE, linear 130 µm/m-°C

@Temperature 23.0 - 100 °C
72.2 µin/in-°F

@Temperature 73.4 - 212 °F
Thermal Conductivity 0.310 W/m-K
2.15 BTU-in/hr-ft²-°F
Melting Point 165 °C
329 °F
DSC, 10°C/min.; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 °C
194 °F
Continuous; 20,000 h
105 °C
221 °F
Continuous; 5,000 h
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
Oxygen Index <= 20 %
<= 20 %
ISO 4589-1/-2
Electrical Properties Metric English Comments
Volume Resistivity >= 1.0e+13 ohm-cm
>= 1.0e+13 ohm-cm
IEC 60093
Surface Resistivity per Square >= 1.0e+12 ohm
>= 1.0e+12 ohm
IEC 60093
Compliance Properties Metric English Comments
3A-Dairy No
No
European Food 1935/2004 Yes
Yes
FDA Yes
Yes
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Unacceptable
Unacceptable
Acids, Weak Limited
Limited
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Acceptable
Alkalies, Weak Acceptable
Acceptable
Chlorinated Solvents Limited
Limited
Continuous Sunlight Limited
Limited
Hot Water / Steam Limited
Limited
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Acceptable
Acceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Acceptable
Acceptable