Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.60 GPa | 377 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CY6120 PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS featuring good flow and impact properties. UL-94 V0 listed at 1.2mm intended for various thin wall applications. |
|||
Tensile Modulus | 2.60 GPa @Thickness 4.00 mm, Temperature 23.0 °C |
377 ksi @Thickness 0.157 in, Temperature 73.4 °F |
Injection Molded; ISO 527-2/50 |
PolyOne Bergamid™ B70 VN4805 LS PM-Z BK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Tensile Modulus | 2.60 GPa @Temperature 23.0 °C |
377 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® 6130 NC010 PBT
(Unverified Data**) Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 2.60 GPa @Temperature 23.0 °C |
377 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® 6134 NC010 PBT
(Unverified Data**) Crastin® 6134 NC010 is an unreinforced, medium viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | 1 mm/min |
Polimeri Europa SINKRAL B23 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,105-04-16-25 High heat resistant grade with good impact resistance. Suitable for injection moulding and extrusi.. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | ASTM D638 |
PolyOne Lubri-Tech™ ATH-000/05M Acetal Homopolymer - 5% MoS2
(discontinued **) Data provided by PolyOne. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer (Asia Pacific) XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo.. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP KP004AXZ ACETAL HOMOPOLYMER LNP* LUBRICOMP* KP004AXZ is a compound based on Acetal Homopolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® HX3061HP PBT PBT for compounding/fibers only. Not intended for injection molding. Biocompatible. Melt viscosity: 250C at 21.6 kgf is 1450-1850 poise. Available in Natural color (1001) only. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP DX11355 PC (Asia Pacific) This is a PC based compound with good plating, surface, mechanical performance and flame retardant (Halogen free), a good candidate for Laser Direct Structuring applications. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | ISO 527-1/-2 |
Styrolution Luran® S KR 2864 C Colored ASA+PC Description: Easy flowing injection molding grade with heat resistance for parts with thin walls and/or with adverse flowpath/wall thickness ratios.Applications: Mobile phone housings.Information pr.. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | ISO 527 |
Styrolution PS 416N HIPS Styrolution PS 416N is medium impact polystyrene with very good flow properties. It has a high rigidity whilst displaying a very good surface gloss.Very good flow propertiesHigh rigidityVery good su.. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQ3001 PBT Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY SLDM2005 PC (Asia Pacific) Antistatic Polycarbonate, Non Halogen FR V-2 grade, mineral 5% filled |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® CE2055 BK580 Polybutylene Terephthalate (PBT) Unreinforced Low Viscosity Polybutylene Terephthalate Crastin CE2055 is an unreinforced low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performanc.. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® FGS600F40 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Food Contact Applications Crastin FGS600F40 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for injection .. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® S600F10 BK851 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin S600F10 BK851 is an unreinforced lubricated medium high viscosity black polybutylene tere.. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | DIN 53 457 |
Hippe PBT Polybutylene Terephthalate The mechanical properties of PBT are generally inferior to the partially crystallized PET, however, PBT is more easily machined.Information provided by Hippe. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | ASTM D638 |
Azdel SuperLite® SL551400-100 PP Resin Matrix / 55% Glass Fiber (4 mm Molded Thickness) AZDEL SuperLite® SL551400-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | ASTM D638 |
PolyOne Lubri-Tech™ MP-000/10T Modified PPO - 10% PTFE
(discontinued **) Data provided by PolyOne. |