Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.55 GPa | 370 ksi | |
Plastcom SLOVALEN PC 53 T 25 PP, 25% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 25% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu.. |
|||
Tensile Modulus | 2.55 GPa | 370 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® SLX2432T PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors. |
|||
Tensile Modulus | 2.55 GPa | 370 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics GELOY XP7550 ASA+PC Injection molding ASA-PC Blend suitable for exterior applications featuring outdoor weatherability, toughness, good heat performance and excellent flow. |
|||
Tensile Modulus | 2.55 GPa | 370 ksi | ASTM D638 |
Ravago Manufacturing Americas Hylac® FR74 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Modulus | 2.55 GPa | 370 ksi | ASTM D638 |
Fiberfil® PP-60/TC/20 Polypropylene Homopolymer, 20% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 2.55 GPa | 370 ksi | 1 mm/min; ISO 527-1,-2 |
Ineos ABS Lustran® ABS 240 Injection Molding Grade Lustran® ABS 240 has standard impact strength and is injection molding grade. |
|||
Tensile Modulus | 2.55 GPa | 370 ksi | |
Ineos ABS Lustran® H606 LS Improved heat and UV resistance.,Property data per ISO test methods. |
|||
Tensile Modulus | 2.55 GPa | 370 ksi | ASTM D638 |
Ineos Styrenics Polystyrene 168M (NAFTA) High heat, high molecular weight general purpose polystyrene with low crystal clarity. It offers high stiffness for extrusion/thermoforming applications, especially for the food packaging.Informati.. |
|||
Tensile Modulus | 2.55 GPa | 370 ksi | ASTM D638 |
Fiberfil® PP-15/T/10/20 Polypropylene Homopolymer, 22% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 2.55 GPa | 370 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP KL002 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KL002 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.55 GPa | 370 ksi | ISO 527 |
Solvay Technyl® A238 Unfilled, Heat Stabilized, Impact Modified Nylon 66 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Tensile Modulus | 2.55 GPa | 370 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
Tensile Modulus | 2.55 GPa | 370 ksi | ASTM D638 |
Star Plastics PC/ABSFR9001 Molding Grade PC/ABSFR Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.55 GPa | 370 ksi | 1mm/min; ISO 527-2 |
Styron EMERGEâ„¢ 7560 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) EMERGEâ„¢ PC/ABS 7560 advanced resin is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. This resin is suitable for use in a wide variety of applications in the.. |
|||
Tensile Modulus | 2.55 GPa | 370 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DX02437 PC (Asia Pacific) LNP Stat-Kon DX02437 is a compound based on Polycarbonate resin containing conductive carbon powder, with good impact-resistance, flow and ESD performance, suitable for semi-con industry. |
|||
Tensile Modulus | 2.55 GPa | 370 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP 9X10401H ABS LNP* THERMOCOMP* 9X10401H is a compound based on Polyphenylsulfone containing proprietary filler(s). Added feature of this grade is: X-Ray Opaque. |
|||
Tensile Modulus | 2.55 GPa | 370 ksi | ASTM D638 |
Ensinger Tecatron® XP-76 Compression Molded PPS Compound, 55% PTFE Filled Seal Material Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Tensile Modulus | 2.55 GPa @Thickness 3.17 mm |
370 ksi @Thickness 0.125 in |
Type I; ASTM D638 |
Calsak CS-72 General Purpose ABS Resin Product Characteristics:High Impact, High GlossInjection molding grade |
|||
Tensile Modulus | 2.55 GPa | 370 ksi | ASTM D-638 |
Axiall ProTherm® 4510 CPVC Rigid PVC, Molding Georgia Gulf ProTherm® 4510 CPVC is a pelletized injection molding compound designed for fittings. Typical applications are in potable water and chemical transfer systems especially where high che.. |
|||
Tensile Modulus | 2.55 GPa | 370 ksi | ISO 527-1/2 |
BLUESTAR BS270 Acetal Copolymer Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Modulus | 2.55 GPa | 370 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ ES-000/15T Polyethersulfone, PTFE Lubricated
(discontinued **) Description/Features:PTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 2.55 GPa | 370 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL ENG265 PPE+PS PPE+PS blend. Unfilled. Suitable for profile extrusion. NSF listed for potable water use in several colors (Standard 61). Low water absorption. Hydrolytic stability. Dimensional stability. Typical a.. |