Category | Polymer , Thermoplastic , Polycarbonate (PC) |
Manufacturer | SABIC Innovative Plastics (GE Plastics) |
Trade Name | Lexan® |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | SABIC Innovative Plastics Lexan® SLX2432T PC Copolymer (Asia Pacific).pdf |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 |
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
Water Absorption | 0.12 % @Time 86400 sec |
0.12 % @Time 24.0 hour |
ASTM D570 |
Moisture Absorption | 0.170 % | 0.170 % | 23°C / 50% RH; ISO 62 |
Water Absorption at Saturation | 0.25 % | 0.25 % | ISO 62 |
Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Melt Index of Compound | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 69.0 MPa | 10000 psi | 50 mm/min; ISO 527 |
72.0 MPa | 10400 psi | Type I, 50 mm/min; ASTM D638 | |
Tensile Strength, Yield | 65.0 MPa | 9430 psi | 50 mm/min; ISO 527 |
67.0 MPa | 9720 psi | Type I, 50 mm/min; ASTM D638 | |
Elongation at Break | 110 % | 110 % | Type I, 50 mm/min; ASTM D638 |
110 % | 110 % | 50 mm/min; ISO 527 | |
Elongation at Yield | 6.0 % | 6.0 % | Type I, 50 mm/min; ASTM D638 |
6.0 % | 6.0 % | 50 mm/min; ISO 527 | |
Tensile Modulus | 2.55 GPa | 370 ksi | 50 mm/min; ASTM D638 |
2.55 GPa | 370 ksi | 1 mm/min; ISO 527 | |
Flexural Yield Strength | 105 MPa | 15200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
105 MPa | 15200 psi | 2 mm/min; ISO 178 | |
Flexural Modulus | 2.50 GPa | 363 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
2.50 GPa | 363 ksi | 2 mm/min; ISO 178 | |
Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
0.980 J/cm @Temperature -30.0 °C |
1.84 ft-lb/in @Temperature -22.0 °F |
ASTM D256 | |
Izod Impact, Unnotched | 26.0 J/cm | 48.7 ft-lb/in | ASTM D4812 |
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*3; ISO 180/1A |
10.0 kJ/m² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A | |
Izod Impact, Unnotched (ISO) | NB | NB | 80*10*3; ISO 180/1U |
Charpy Impact Unnotched | NB | NB | Edgew 80*10*3 sp=62mm; ISO 179/1eU |
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
1.50 J/cm² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA | |
Dart Drop, Total Energy | 77.0 J @Temperature 23.0 °C |
56.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
85.0 J @Temperature -40.0 °C |
62.7 ft-lb @Temperature -40.0 °F |
ASTM D3763 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
CTE, linear, Transverse to Flow | 64.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
64.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
Deflection Temperature at 0.46 MPa (66 psi) | 130 °C | 266 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
130 °C @Thickness 3.20 mm |
266 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
Deflection Temperature at 1.8 MPa (264 psi) | 116 °C | 241 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
118 °C @Thickness 3.20 mm |
244 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
Vicat Softening Point | 135 °C | 275 °F | Rate B/50; ASTM D1525 |
135 °C | 275 °F | Rate B/50; ISO 306 | |
137 °C | 279 °F | Rate B/120; ISO 306 | |
Flammability, UL94 | V-2 @Thickness 1.50 mm |
V-2 @Thickness 0.0591 in |
UL 94 |
Oxygen Index | 38 % | 38 % | ISO 4589 |
Glow Wire Test | 960 °C @Thickness 1.60 mm |
1760 °F @Thickness 0.0630 in |
IEC 60695-2-12 |
Optical Properties | Metric | English | Comments |
---|---|---|---|
Refractive Index | 1.59 | 1.59 | ASTM D542 |
Haze | 0.80 % @Thickness 2.54 mm |
0.80 % @Thickness 0.100 in |
ASTM D1003 |
Transmission, Visible | 84 % | 84 % | 2.54 mm; ASTM D1003 |
Descriptive Properties | Value | Comments |
---|---|---|
Ball Pressure Test, 125°C +/- 2°C | PASSES | IEC 60695-10-2 |
UV-light, water exposure/immersion | F1 | UL 746C |