Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.47 GPa | 358 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging 2320 LCW Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.47 GPa | 358 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® MG37EPX ABS ABS plating grade optimized for a broad processing window for both painted and plated applications. NSF standard 61 compliant (80 sq in/L) |
|||
Tensile Modulus | 2.47 GPa | 358 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Geloy XTWE480 ASA (Asia Pacific) Anti-scratch Geloy grade with excellent weatherability, high flow, and good surface quality. XTWE480 is available in various colours.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 2.47 GPa | 358 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP COLORCOMP D10006U PC LNP* COLORCOMP* D10006U is an unfilled Polycarbonate. Added features include: Lasermarking Capability, UL Listed. |
|||
Tensile Modulus | 2.47 GPa | 358 ksi | ISO 527-2 |
Solvay Specialty Polymers Ixef® BXT-2000/0203 Polyarylamide (PARA)
(Unverified Data**) Ixef BXT-2000/0203 resin was developed specifically for extrusion and blow-molding processes. Unlike grades targeted for injection molding, Ixef BXT-2000/0203 resin can be successfully extruded into.. |
|||
Tensile Modulus | 2.47 GPa @Thickness 3.20 mm |
358 ksi @Thickness 0.126 in |
1mm/min; ASTM D638 |
LG Chemical HIPS MI730 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Tensile Modulus | 2.47 GPa | 358 ksi | ASTM-D638 |
Ineos ABS Lustran® Guardian™ 682 ABS, Injection Molding Grade Lustran® ABS 682 is a high performance, HCFC-141b resistant grade of ABS for injection molded refrigerator and freezer components. |
|||
Tensile Modulus | 2.47 GPa | 358 ksi | ISO 527-2 |
Solvay Specialty Polymers Ixef® BXT 2000-0203 Polyarylamide (PARA) Ixef® BXT 2000-0203 resin was developed specifically for extrusion and blow-molding processes. Unlike grades targeted for injection molding, Ixef® BXT 2000-0203 resin can be successfully extru.. |
|||
Tensile Modulus | 2.47 GPa | 358 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DX04462C PC LNP STAT-KON* DX04462C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive. |
|||
Tensile Modulus | 2.47 GPa | 358 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PVX516 PPE PREVEX* PVX516 resin is a high flow, non FR grade, 110 C HDT |
|||
Tensile Modulus | 2.47 GPa | 358 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DX04462C PC (Asia Pacific) LNP* STAT-KON* DX04462C is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Clean Compounding System. |
|||
Tensile Modulus | 2.47 GPa | 358 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts.. |
|||
Tensile Modulus | 2.47 GPa | 358 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER (Asia Pacific) Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts.. |
|||
Tensile Modulus | 2.47 GPa | 358 ksi | 1mm/min |
Eastman Eastapak 9921 PET ISO data as provided by the manufacturer, Eastman Chemical |
|||
Tensile Modulus | 2.47 GPa | 359 ksi | Storage |
Epoxy Technology EPO-TEK® OE101 Two Component Epoxy Material Description: A two component epoxy designed for low stress applications in fiber optic packaging, opto-electronics and semiconductors. It is a lower modulus version of EPO-TEK® 353ND.Inf.. |
|||
Tensile Modulus | 2.47 GPa @Temperature 80.0 °C |
358 ksi @Temperature 176 °F |
ISO Data |
BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Dry) Ultramid 8231G HS is a heat stabilized, 14% glass fiber reinforced nylon 6 injection molding compound. It is also available in non-heat stabilized (Ultramid 8231) and/or pigmented versions. The gla.. |
|||
Tensile Modulus | 2.47 GPa | 358 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen.. |
|||
Tensile Modulus | 2.47 GPa | 358 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS (Asia Pacific) Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen.. |
|||
Tensile Modulus | 2.47 GPa | 358 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen.. |
|||
Tensile Modulus | 2.47 GPa | 358 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER (Europe-Africa-Middle East) Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts.. |