Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.45 GPa | 355 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion 85857 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding 6957 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Geloy FXTW26SK ASA Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® CFR9712 PC COPOLYMER (Europe-Africa-Middle East) Lexan* CFR9712 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 2.0 mm and high flow capability. .. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® DMX2415 PC (Asia Pacific) Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Asia P.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer (Europe-Africa-Middle East) Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EX2079X PC (Europe-Africa-Middle East) Lexan* EX2079X polycarbonate resin, MVR (300°C/1.2kg) 3 cm3/10min, high viscosity, branched, extrusion, flame retardant, halogen free per DIN VDE 0472 Part 815, mold release, UV stabilized, translu.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EX7631T PC EX7631T is a high UVA content homopolymer polycarbonate product intended for use as a cap layer for polycarbonate sheet extrusion. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HPB3144G PC Copolymer Standard flow, transparent, high purity polycarbonate copolymer resin with reduced oxygen permeability and water vapor transmission rate. For medical devices and pharmaceutical applications. Health.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® CFR9712 PC COPOLYMER (Asia Pacific) Lexan* CFR9712 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 2.0 mm and high flow capability. .. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer (Asia Pacific) This product will be phased out per January 2015 -- Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HPS7 PC (Asia Pacific) Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | (1mm/min); ISO 527-2/1A |
Aardvark Polymers AARTEL® 100 D/S Rotational Molding Resin Aartel 100SD is a new conductive grade developed to dissipate electricity in fuel handling systems. Aartel 100SD maintains all o the excellent properties of our general purpose acetal, has a volume .. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics SABIC PPCOMPOUND 37T1020 PP SABIC® PPcompound 37T1020 is a general purpose, talc filled, heat stabilized copolymer polypropylene compound. This compound exhibits high impact and high flow, and is suitable for injection mold.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics SABIC PPCOMPOUND 55T1040 PP SABIC® PPcompound 55T1040 is a general purpose, talc filled, heat stabilized copolymer polypropylene compound. This compound exhibits very high impact and high rigidity, and is suitable for injec.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DSL229 PC (Asia Pacific) LNP* Stat-kon* DSL229 is a compound based on Polycarbonate resin containing PTFE, Stainless Steel. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1mm/min; ISO 527 |
Teijin Multilon T-3011 Standard PC/ABS Polymer Alloy General grade of PC/ABS polymer alloy, having improved impact strength and heat resistance compared with a heat resistant ABS and flame retardant m-PPE and also having higher fluidity compared with .. |
|||
Tensile Modulus | 2.45 GPa | 356 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® BF-0679P MABS, Unreinforced Scratch Resistant Scratch resistant material that is used for the exterior material of flat TVInformation provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL EXNL0303 PPE+HIPS (Europe-Africa-Middle East) EXNL0303 is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nor.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1mm/min; ISO 527-2 |
Borealis Daplen™ EF267AI Polypropylene TPO Compound Daplen™ EF267AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process... |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | ISO 527-1/-2 |
Covestro Makrolon® 6457 Polycarbonate, Flame Retardant Grade MVR (300 °C/1.2 kg) 12.5 cm3/10 minUL 94V-0/3.0 mmUV stabilizedeasy releaseinjection moldingavailable in transparent, translucent and opaque colorsPreprocessingMax. Water content |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1mm/min; ISO 527-1 |
Denka MALECCA K-300 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | ISO 527-1/-2 |
Covestro Makrolon® 6487 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minFlame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmMedium viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 2.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | |
Dow SiLK™ I300 140 Semiconductor Dielectric Resin SiLK™ I300 140 is designed for easy integration and extendibility, and its formulations offer a robust feature set. High thermal stability and fracture toughness means SilK™ I300 140 is compatibl.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min |
Arkema Group Orgalloy® R 6600 Nylon 66 Alloy, Rigid Grade (Conditioned) Rigid polyamide 6.6 alloy: easy to process, low moisture absorption, chemical resistance (no known solvents).ISO data provided by the manufacturer, Arkema. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | ISO 527-1/2 |
BLUESTAR BS090 Acetal Copolymer Information provided by Polymer Technology and Services, LLC (PTS). |