Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.13 GPa | 309 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® EX75 ABS Multi-purpose, extrusion ABS providing a favorable balance of engineering properties. |
|||
Tensile Modulus | 2.13 GPa | 309 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® MG34LG ABS Automotive: Low gloss ABS for unpainted interior applications. |
|||
Tensile Modulus | 2.13 GPa | 309 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Cycolac® MG34LGHF ABS Low gloss, high flow ABS for unpainted interior applications.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.13 GPa | 309 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® MG38F ABS Very high impact ABS. Toughness/rigidity. FDA compliant. |
|||
Tensile Modulus | 2.13 GPa | 309 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® MG38F ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. FDA compliant. |
|||
Tensile Modulus | 2.13 GPa | 309 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® MGABS02 ABS General purpose ABS. Excellent flow/impact. |
|||
Tensile Modulus | 2.13 GPa | 309 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® MC1300 PC+ABS Cycoloy MC1300 resin is an injection moldable PC/ABS blend with excellent flow and impact performance. It is designed for plating applications mostly used in the automotive industry. |
|||
Tensile Modulus | 2.13 GPa | 309 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® MC1300 PC+ABS (Asia Pacific) Cycoloy MC1300 resin is an injection moldable PC/ABS blend featuring excellent flow and impact performance. It is designed for plating applications mostly used in automotive industry. |
|||
Tensile Modulus | 2.13 GPa | 309 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HP9NR PC Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. For blow molding .. |
|||
Tensile Modulus | 2.13 GPa | 309 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS (Asia Pacific) LNP* LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.13 GPa | 309 ksi | |
Ineos ABS Lustran® LGA-SF
(discontinued **) Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquir.. |
|||
Tensile Modulus | 2.13 GPa | 309 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS LNP LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.13 GPa | 309 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS (Europe-Africa-Middle East) LNP* LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.13 GPa | 309 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DP001E PC LNP* LUBRICOMP* DP001E is a Polycarbonate base resin containing 5% PTFE/Silicone. Added features are: Internally Lubricated, Easy Molding. |
|||
Tensile Modulus | 2.13 GPa | 309 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DX09407H PC LNP* LUBRICOMP* DX09407H is a compound based on High Heat Polycarbonate containing proprietary fillers. Added features of this grade are: Wear Resistant, Healthcare. |
|||
Tensile Modulus | 2.13 GPa | 309 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP KL004 Acetal Copolymer LNP LUBRICOMP* KL004 is a compound based on Acetal Copolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 2.13 GPa | 309 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP KL004 Acetal Copolymer (Asia Pacific) LNP Lubricomp* KL004 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated. This grade was previously found under the LNP* Fu.. |
|||
Tensile Modulus | 2.13 GPa | 309 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP KL004 Acetal Copolymer (Europe-Africa-Middle East) LNP* LUBRICOMP* KL004 is a compound based on Acetal Copolymer containing PTFE. Added features include Internally Lubricated. |
|||
Tensile Modulus | 2.13 GPa | 309 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP KL004XXC Acetal Copolymer LNP LUBRICOMP* KL004XXC is a compound based on Acetal Copolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 2.13 GPa | 309 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp DX93681 PC LNP* Thermocomp* DX93681 is a compound based on Polycarbonate resin containing Proprietary Filler(s).This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.13 GPa | 309 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp DX93681 PC (Asia Pacific) LNP* Thermocomp* DX93681 is a compound based on Polycarbonate resin containing Proprietary Filler(s).This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 2.13 GPa | 309 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.13 GPa | 309 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 (Europe-Africa-Middle East) High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 2.13 GPa | 309 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PN275F PPE+PS PPE+PS with low mineral loading. High heat, platable applications. NSF approved for water contact applications. |
|||
Tensile Modulus | 2.13 GPa | 309 ksi | ISO 527 |
Polyram RamTough PZ509 Polycarbonate, Easy Flow, Flame Retardant Non-transparent polycarbonate, easy flow, flame retardant, for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 2.13 GPa | 309 ksi | ISO 527 |
Polyram RamTough PZ513 Polycarbonate, Easy Flow, Flame Retardant Transparent polycarbonate, UV stabilized, easy flow, flame retardant, for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 2.13 GPa | 309 ksi | 1mm/min |
Eastman Eastar DN001 PCTG Copolyester ISO data as provided by the manufacturer, Eastman Chemical |
|||
Tensile Modulus | 2.13 GPa @Temperature -20.0 °C |
309 ksi @Temperature -4.00 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® ST801 BK010A Nylon 66
(Unverified Data**) Super Toughened Polyamide 66 Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 2.13 GPa | 309 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 49 Nylon 66, Impact Modified, Conditioned Vydyne® 49 is general-purpose, impact-modified PA66 resin. Available in natural, is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact s.. |
|||
Tensile Modulus | 2.13 GPa | 309 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 49H NT Nylon 66, Impact Modified, Conditioned Vydyne® 49H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat-stabilized for improved resista.. |