Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.00 GPa | 290 ksi | Mixed 1:1; TM R050-36 |
Resinlab® EP1215 Clear Unfilled Epoxy Structural Adhesive Resinlab™ EP1215 Clear is a two part unfilled epoxy structural adhesive designed for bonding applications requiring high strength and good impact resistance. It cures completely at room temperature.. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | |
Plastcom SLOVALEN PQ 81 T 25 PP, 25% mineral filling FeaturesModified PP for injection moulding with the content of 25% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shri nkage. Gen.. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | STN EN ISO 527-2 |
Plastcom SLOVASTYR® B BT N PBT Regranulate PBT basic type for injection molding. Melt is characterized by very good fluidity, which enables injection molding of complicated and divided products also on multiple moulds. Anisotropy.. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL9134 PC Copolymer Lexan* EXL9134 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, .. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | 2.0 in/min; 0.050" thickness; ASTM D-638 |
Chevron Phillips EB6025 HIPS - High Impact Polystyrene
(discontinued **) Rubber modified high impact polystyrene.Applications:Cosmetic packagingShower surroundsPoint of purchase displaysThin-wall injection molding and thermoformingFeatures:Smooth, glossy surface finishGo.. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | 1 mm/min; ISO 527 |
Polimeri Europa Edistir RKL Polystyrene
(discontinued **) UL94 V-0, flame retarded, high impact polystyrene. This grade is designed for the extrusion of flame retardant sheets, foils and profiles. Designation: Thermoplastics ISO 2897-PS-I,E,093-06-04-18App.. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | 1 mm/min; ISO 527-1,-2 |
Ineos ABS Lustran® Ultra 4105 ABS Pellets (Polycarbonate-modified), Medium High Heat Grade Lustran® Ultra 4105 is medium high heat grade with superior impact resistance. It is PC-modified and has low emission. It is used for the production of molded plastic articles. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | ISO 527 Type 1A |
Solvay TECHNYL® C 50 H2 PA6, Conditioned Description: TECHNYL® C 50H2 is a unreinforced melamine cyanurate flame retarded polyamide 6. This product is heat stabilized and can be used for injection molding and extrusion processes. This p.. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQ357M PBT+PC Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xylex X7200 PC+POLYESTER (Europe-Africa-Middle East) General purpose, UV stabilised Xylex gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | ASTM D 638 |
Styrolution PS 6210/6211 HIPS Great balance of rigidity and toughnessUSP Class VI certifiedUL Classification 94 HBInformation provided by Styrolution |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | ISO 527 |
Styrolution PS 641F HIPS Styrolution PS 641F is high impact polystyrene with high heat resistance.High impactHigh heat resistanceInformation provided by Styrolution |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | At 1 mm/min; ISO 178 |
Borealis Borcoat™ GA700E-7032 Syntactic Polypropylene for Steel Pipe Coating Borcoat GA700E-7032 is a grey colored syntactic, high impact polypropylene with high thermal insulation capacity and high compressive strength.Borcoat GA700E-7032 is recommended as thermal insulatio.. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | ISO 527 |
Polyram RamLloy PBB704 PC/ABS Alloy, UV Stabilized PC/ABS alloy, UV stabilized, for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | ISO 527 |
Polyram PlusTek PB340S50 Nylon 6 for Injection Molding, 50% Glass-beads Reinforced, Heat Stabilized 50% Glass-beads reinforced, heat stabilized Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | 1 mm/min; ISO 527-1,-2 |
Covestro Makroblend® UT5207 PC/PBT Blend Main characteristics:• High toughness even at low temperatures• Good chemical resistance• Good paintability• Good flowability• Low moisture intakeGrade characteristics:• Impact modified•.. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide P1000IX3 PA6, Impact Modified, Injection Molded Staramide P1000IX3 is an Impact Modified, Polyamide 6 Injection Molding Resin (also known as P1000HI020 or Star X 2020)Information provided by Eurostar. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 300TE NC010 Acetal (POM)
(Unverified Data**) Toughened Medium-high Viscosity Acetal Homopolymer with Very Low EmissionsDelrin 300TE NC010 is a medium-high viscosity toughened acetal homopolymer with very low VOC emissions. Processing methods i.. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | ASTM D638 |
Aclo Accucomp ABS ABS881L Clear Grade |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | ISO 527-1 |
Barlog Plastics KEBAFORM C 901 SO POM Copolymer unreinforced, improved wear and friction POMInformation provided by BARLOG plastics GmbH. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | At 1 mm/min; ISO 527-2 |
Borealis Xmod™ MC55T1 Polypropylene Compound 10% Mineral Filled Xmod MC55t1 is a 10% mineral filled grade based on HCPP intended for injection molding. Xmod has been developed especially for the car industry, to be used in interior parts. XMod offers very good .. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | ASTM D638 |
Spartech Solarex® K High Heat Weatherable Copolyester Sign Grade Sheet Information provided by Spartech. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | ASTM D638 |
ExxonMobil Paxon™ AS55-003 Blow Molding Resin
(discontinued **) AS55-003 is a blow molding grade high density polyethylene copolymer containing an antistat additive. It provides a good balance of stiffness and stress crack resistance.Information provided by Exx.. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® CL101D PBT+PC (Europe-Africa-Middle East) XENOY CL101D is an impact modified PBT+PC injection moulding resin with excellent low temperature impact performance. Applications: automotive exterior components such as bumper systems.This data wa.. |