Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 11.7 GPa | 1700 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Stat-Tech™ AT-10CF/000 Acetal (POM) Copolymer Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Tensile Modulus | 11.7 GPa | 1690 ksi | ASTM D638 |
Polymer Resources PEI-G40 Polyetherimide, 40% Glass Reinforced Polyetherimide, 40% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
Tensile Modulus | 11.7 GPa | 1700 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® PS-30GF/000 FR V0 Polybutylene Terephthalate (PBT), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedFlame RetardantPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 11.7 GPa | 1700 ksi | ASTM D638 |
LNP Stat-Kon® PDX-E-99689 CCS Polyetherimide, Carbon Fiber Reinforcement
(discontinued **) Features: Low to None Ion Content, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued.. |
|||
Tensile Modulus | 11.7 GPa | 1700 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 60 G1 V30 PA66, 30% glass fiber, DRY Description: Flame retardant Polyamide PA66 reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This R.. |
|||
Tensile Modulus | 11.7 GPa | 1700 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon EE005 PEI (Asia Pacific) LNP STAT-KON* EE005 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the .. |
|||
Tensile Modulus | 11.7 GPa | 1700 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON EE005E PEI (Asia Pacific) LNP STAT-KON* EE005E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Tensile Modulus | 11.7 GPa | 1700 ksi | ISO 527 |
Polyram PlusTek PA313G43 Nylon 66 for Injection Molding, 43% Glass Fiber Reinforced, Heat Stabilized Heat stabilized, 43% Glass fiber reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 11.7 GPa | 1700 ksi | ASTM D638 |
Applied Composites 8072 Polyester SMC Industry Application: TransportationProduct Application: AutomotiveDistinct Features: Zero Shrink, Superior Class A Finish, Improved Impact, Accepts Mold CoatingInformation provided by Applied Compo.. |
|||
Tensile Modulus | 11.7 GPa | 1700 ksi | 1mm/min; ISO 527 |
BASF Ultradur B 4406 G6 BKQ113 7110 30% Glass Filled PBT Ultradur B 4406 G6 BKQ113 7110 is an UL V0 injection molding, pigmented black, PBT grade with 30% glass fiber reinforcement. |
|||
Tensile Modulus | 11.7 GPa | 1700 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer Amodel AS-4133 HN polyphthalamide (PPA) is a non-lubricated, heat stabilized grade that offers fast cycle times and is hot-water moldable. Typical applications include electrical and electronic comp.. |
|||
Tensile Modulus | 11.7 GPa | 1700 ksi | |
Radici Radiflam® A RV300AE (cond.) Nylon 66-30GF PA66 flame retardant injection molding grade. 30% Glass fiber reinforced, for items with high stiffness. Natural colorInformation provided by Radici group. |
|||
Tensile Modulus | 11.7 GPa | 1700 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® A-4133 L Polyphthalamide (PPA), Dry
(discontinued **) Amodel A-4133L polyphthalamide (PPA) is a 33% glass reinforced resin designed to offer high crystallinity when molded in water-cooled molds. Key properties include high heat resistance, reduced outg.. |
|||
Tensile Modulus | 11.7 GPa | 1700 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Conditioned
(discontinued **) Availability: Asia Pacific; Europe; North AmericaInformation provide by Solvay Specialty Polymers |