Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 10.7 GPa | 1550 ksi | |
Idemitsu Kosan Xarec® EA 513 SPS, 30% Glass Filled |
|||
Tensile Modulus | 10.7 GPa | 1550 ksi | |
Idemitsu Kosan Xarec® EA 533 SPS, 30% Glass Filled Glass Filled, Ignition Resistant, Impact Modified. Used in electronic and electrical applications. |
|||
Tensile Modulus | 10.7 GPa | 1550 ksi | ISO 527 Type 1A |
Solvay TECHNYL® CR 218 V33 Black 21 N Nylon 6, 30% glass fiber, DRY Description: Polyamide PA6 reinforced with 33% of glass fiber, heat stabilized, containing recycled material.Available in: North AmericaProduct Applications: This grade is suitable for none critical.. |
|||
Tensile Modulus | 10.7 GPa | 1550 ksi | ISO 527 Type 1A |
Solvay TECHNYLSTARâ„¢ S 216 V35 PA6, 35% glass filled, DRY Description: TECHNYLSTAR polyamide, reinforced with 35% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Europe and North AmericaProduct Applications.. |
|||
Tensile Modulus | 10.7 GPa | 1550 ksi | ISO 527 Type 1A |
Solvay TECHNYLSTARâ„¢ S 218 V35 PA6, 35% glass filled, DRY Description: TECHNYL STAR Polyamide, reinforced with 35% of glass fiber, heat stabilized, for injection molding. Characterized by a high fluidity of the melt. Available in: Europe and North America .. |
|||
Tensile Modulus | 10.7 GPa | 1550 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 553 PBT (Europe-Africa-Middle East) VALOX 553 is a 30% glass fibre reinforced, flame retardant PBT+PC blend with good warpage characteristics. Applications: appliance handles, spotlights, electric motors, pumphousings. |
|||
Tensile Modulus | 10.7 GPa | 1550 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® IQ420 PBT Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
Tensile Modulus | 10.7 GPa | 1550 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® IQ420 PBT (Asia Pacific) Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
Tensile Modulus | 10.7 GPa | 1550 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® IQ420 PBT (Europe-Africa-Middle East) Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
Tensile Modulus | 10.7 GPa | 1550 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® IQ420HP PBT (Asia Pacific) Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
Tensile Modulus | 10.7 GPa | 1550 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® IQ4860HR PBT Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
Tensile Modulus | 10.7 GPa | 1550 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® IQ4860HR PBT (Asia Pacific) Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
Tensile Modulus | 10.7 GPa | 1550 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® IQ4860HR PBT (Europe-Africa-Middle East) Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
Tensile Modulus | 10.7 GPa | 1550 ksi | ASTM D638 |
Plenco 1500 Polyester, Granular, Transfer Molded PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under compon.. |
|||
Tensile Modulus | 10.7 GPa | 1550 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA) 30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide with Improved Flow Zytel HTNFR52G30NHF BK337 is a 30% glass reinforced flame retardant lubricated high performance.. |
|||
Tensile Modulus | 10.7 GPa | 1550 ksi | ASTM D638 |
Plenco 6527 Phenolic, Granular, Injection Molded PLENCO 06527 is a woodflour and mineral filled resole phenolic molding compound.Information supplied by Plenco. |
|||
Tensile Modulus | 10.7 GPa | 1550 ksi | ASTM D638 |
DuPont Performance Polymers Rynite® 530HTE NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Polyethylene Terephthalate with Excellent High Temperature Dielectric PropertiesRynite 530HTE NC010 is a 30% glass reinforced modified polyethylene terephthalate resin with exce.. |