Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.90 GPa | 276 ksi | ISO.527 DIN.53455 |
Omnia Plastica Omniamid PA6 GHR - HR - at 50% RH Cast nylon 6 produced with the addition of graphite and a special lubricator which gives to this product better properties than natural PA6G. Whilst retaining the general features of OMNIAMID G it i.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ASTM Data |
Americas Styrenics Styron® XL-8028 High Impact Polystyrene
(discontinued **) STYRON® XL-8028 high impact polystyrene is designed for VCR cassettes, toys, small appliances, telephones, housewares, tool items, computer consoles and bodies for computer cartridges. It offers hi.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | |
Ineos ABS Lustran® QE 1006, Extrusion Grade
(discontinued **) Extrusion grade with high impact.Applications: High impact plates.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majo.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1 mm/min |
Polimeri Europa SINKRAL C333/m² ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,105-04-16-20 Special low gloss grade for injection moulding which combines medium heat resistance with a good b.. |
|||
Tensile Modulus | 1.90 GPa | 275 ksi | ASTM D638 |
Fiberfil® PP-61/TC/20 Polypropylene Copolymer, 20% Talc Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ASTM D638 |
Metton LMR M1534 Liquid Molding Resin Different product numbers represent different formulations for customer specific needs such as liquid freezing point. Metton LMR is a tough and durable engineering plastic material used to produce .. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | |
Ineos ABS Triax® KU 2-3050 ABS + Polyamide Blend (DAM) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightHeat stabilized or stable to heatSuitable processing methods:Injection molding |
|||
Tensile Modulus | 1.90 GPa @Temperature 23.0 °C |
276 ksi @Temperature 73.4 °F |
|
LATI Latene® 11 MDT05-01 PP Homopolymer Polypropylene homopolymer (PPh) based compound. Magnetic detectable filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industr.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | |
LATI Latimass 63-06 D025 PA66 Specific density compound based on Polyamide 66 (PA66). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Asia Pacific) XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Asia Pacific reg.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC (Europe-Africa-Middle East) Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics XYLEX X8419 PC+POLYESTER (Asia Pacific) Low-medium flow, suitable for blow molding, injection molding, extrusion. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics XYLEX X8419 PC+POLYESTER (Europe-Africa-Middle East) Low-medium flow, suitable for blow molding, injection molding, extrusion. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Asia Pacific) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL IN120 PPE+HIPS (Europe-Africa-Middle East) NORYL IN120 is an unfilled material with a Vicat B/120 of 125 °C according ISO 306. NORYL IN120 has been developed for the interior automotive |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ISO 527 |
Styrolution Terlux® 2812 HD MABS Description: Terlux 2812 HD is a suitable grade for the food packaging and health care and diagnostic markets.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ASTM D638 |
Lubrizol Isoplast® 2530 Engineering Thermoplastic Polyurethane Resin for Medical Applications Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1mm/min; ISO 527 |
Borealis Daploy™ WB180HMS Polypropylene Daploy™ WB180HMS is a propylene-based, structurally isomeric polymer.Information provided by Borealis AG |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ASTM-D790 |
Polyram RamShine PAS100 ASA, General Purpose General purpose injection molding ASAInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ASTM D638 |
Goodfellow TPX® RT31XB Injection Molding Grade Polymethylpentene This grade is highly recommended for injection molding; also for film and fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release c.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ASTM D638 |
Eastman Eastar EB062 Copolyester Eastar Copolyester EB062 is a resin specifically developed for extrusion blown bottles where aesthetics such as high clarity and gloss, coupled with design flexibility, drive demand. Compared to com.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | Film T.D.; ASTM D882 |
Eastman GSP01 Copolyester for Film and Sheet Extrusion Applications:Consumer e-packaging trayElectronic packagingElectrostatic dissipative trayProduct Description: GSP01 is a clear, amorphous material. Because of its clarity, toughness and good melt s.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ISO 527-2/50 |
ExxonMobil Exxtral™ CMU 101D Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for automotive interior trim in which good surface finish, high scratch resistance, minimum dust deposit and good UV resistan.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | Storage |
Epoxy Technology EPO-TEK® EJ2189 Electrically Conductive Epoxy Product Description: EPO-TEK® EJ2189 is an electrically conductive, silver-filled epoxy paste. This two component system is designed for low temperature curing from ambient to 80°C, although othe.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | |
BASF Polystyrol® 585 K Impact Grade Polystyrene (Europe) Special high gloss, high-impact grade for all types of housings. Basis product for gloss capping.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | |
BASF Procom® D 1195 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 GS 25 HWCP 25% Glass Sphere Filled Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TR 55 LY PA12/MACMI Product description: Grilamid TR grades are transparent thermoplastic polyamides based on aliphatic and cycloaliphatic blocks. Grilamid TR 55 LY offers a variety of interesting properties such as: c.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 67R Nylon 66, Heat Stabilized, Conditioned Vydyne® 67R is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 67R resin offers high strength, .. |