Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.00 GPa | 145 ksi | ISO 527-1/2 |
Radici Radilon® SLVHPL128 (dry) Nylon 6 Plasticized for improved flexibilityInformation provided by Radici group. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | |
Plastcom SLOVAMID 6 GF 25 FRA 5 LS PA6, 25% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 25% glass fibre, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°C,.. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | ASTM D638 |
Ineos ABS Lustran® 456 Extrusion, Matte-Gloss
(discontinued **) Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | |
Ineos ABS Lustran® 2710, Extrusion Grade
(discontinued **) Extrusion grade, for coextrusion to surfaces with extreme low gloss.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a ma.. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | 1% Secant, 50mm/min; ASTM D638 |
LyondellBasell Alathon® H5220 High Density Polyethylene, Injection Molding Grade ApplicationsAlathon H5220 provides easy processing characteristics and exhibits excellent toughness properties and color as well as low odor and good processing stability. Typical applications inclu.. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | 1 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 2-5000 Polypropylene Block-Copolymer INNOPOL® CS 2-5000 is a polypropylene block-copolymer compound. This grade is available in nature and custom colored form.INNOPOL® CS 2-5000 is developed for producing injection molded automot.. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | ISO 527-1 |
Iran Petrochemical (PCC) HB5020 High Density Polyethylene HB-5020 is a high molecular weight high density polyethylene.Applications: extrusion blow moldingInformation provided by Iran Petrochemical Commercial Co. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | conditioned, 1 mm/min; ISO 527-1,-2 |
Lanxess Durethan® BC 30 S 000000 Nylon 6 PA 6, non-reinforced, injection moldingInformation provided by LANXESS. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY KX09024 ACETAL COPOLYMER (Europe-Africa-Middle East) LNP* Statloy* KX09024 is a compound based on Polyacetal with reduced Resistivity. Added features include: Antistatic Properties |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | 1mm/min; ISO 527-2 |
Borealis Daplen™ EE108U Polypropylene TPO Compound Daplen™ EE108U is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, gives.. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | ISO 527 |
Total Lumicene® mPE M5220 Metallocene High Density Polyethylene This product is a Total Ecosolutions grade.Lumicene® mPE M 5220 is a High Density Polyethylene with very good organoleptic properties, dimensional stability, stress-cracking resistance, rigidity an.. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | ISO 527-2 |
Total PPM R021 Polypropylene, Random Copolymer for Medical Grade Polypropylene PPM R021 is a random copolymer polypropylene with a Melt Flow Index of 1.8 g/10 min specially developed for the extrusion blow molding of medical containers and medical devices, to the.. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | ASTM D 638 |
Cossa Polimeri ESTAPROP KUR 1010 TG05 Polypropylene, 5% Mineral Filled PP copolymer 5% mineral fillerElastomer modified, very high impact strength at low temperatureInformation provided by Cossa Polimeri S.r.l. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | ISO 527-1/-2 |
DSM Akulon® F223-D (Cond.) Low/Medium Viscosity Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | ISO 527-1/-2 |
DSM Arnitel® EL740 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | cond; ISO 527-1/-2 |
DSM Stanyl® TS300 PA46 |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000/50 CP Nylon 6, Impact Modified Until 0°C, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | ISO 527-1/-2 |
DSM Stanyl® TW371 Nylon 46 (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 25 NZ ESD PA12 Product Description: Grilamid L 25 NZ ESD is a high viscosity, anti-static extrusion grade of Polyamide 12 (PA12). Grilamid L 25 NZ ESD is impact modified and heat stabilized. The inherent color of .. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | ISO 527-2 |
Domo 2600PC Polypropylene Copolymer Information provided by Domo. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | ASTM D 638 |
Cossa Polimeri ESTAPROP KUR 1520 TG05 Polypropylene, 10% Mineral Filled PP copolymer 10% mineral fillerElastomer modified, very high impact strength at low temperatureInformation provided by Cossa Polimeri S.r.l. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437W10L Wollastonite Reinforced |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | |
BASF Novolen® 2600 PC Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | 1mm/min; ISO 527 |
BASF Ultramid® B50L 01 PA6 (Conditioned) Ultramid B50L 01 is a high-viscosity, lubricated, general-purpose extrusion PA6 grade. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendat.. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | ASTM D638 |
Aclo Accutech Polyethylene HD0204UVL High Density UV Stabilized |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | ASTM D638 |
Aclo Accutech Polypropylene CP0409HUUVV Copolymer UV Stabilized Approved to Suzuki PP-S3 Med Grey T01 |
|||
Tensile Modulus | 1.00 GPa @Temperature 23.0 °C |
145 ksi @Temperature 73.4 °F |
|
LATI Lastane 50 G/25 PUR, 25% Glass Fiber Reinforced Polyurethane (PUR) based compound. Glass fibers. Very good noise reduction. Good impact resistance even at low temperature.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | dry; ISO 527-1/-2 |