Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 52.0 MPa | 7540 psi | ISO 527-2 |
Ravago Manufacturing Americas Hybrid S464LGUV Acrylonitrile Butadiene Styrene + PC Alloy Available in North America UV Stabilizer Good Toughness Low Gloss RoHS Compliant Form: Pellets Processing Method: Injection Molding Automotive Specifications: Chrysler MS-DB300 CPN4352 Color:.. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | ISO 527, ASTM D638 |
Nilit Nilamid A3 H ZC High Impact PA66 Description: Nilamid A3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, .. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | |
Ineos ABS Lustran® QE 1045 A, Injection Grade
(discontinued **) Injection molding grade, high modulus, only available in black.Applications: For automotive application.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed.. |
|||
Tensile Strength, Yield | 52.0 - 56.0 MPa | 7540 - 8120 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 3208/0150 Anti-friction PVDF Compound
(discontinued **) Key features of this grade: Anti-friction, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta.. |
|||
Tensile Strength, Yield | 52.0 MPa @Thickness 3.20 mm |
7540 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical GPPS 25SP(E) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
Tensile Strength, Yield | 52.0 MPa @Thickness 3.20 mm |
7540 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical Lupox® GP1000W PBT Description: Injection Molding, PBT, Anti-HydrolysisApplication: IT/OA, Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | ISO 527-1/-2 |
Mitsubishi Xantar® MX 1021 FD MX 1021 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DX94375H PC LNP* LUBRICOMP* DX94375H is a compound based on Polycarbonate resin containing Proprietary Fillers. Added features of this material include: Healthcare, Wear Resistant. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | SABIC - Japan Method |
SABIC Innovative Plastics Xenoy® RCX201 PC+PET (Asia Pacific) |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Europe-Africa-Middle East) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® HP-1011 PC/ABS, Unreinforced Material with superior flowability and small gas generation that can be used in the exterior material of mobile phonesInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® TF-0956 HI-PMMA Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | ISO 527 |
SABIC Innovative Plastics LNP Thermocomp MX88073 PP LNP* Thermocomp* MX88073 is a compound based on Polypropylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | SABIC - Japan Method |
SABIC Innovative Plastics NORYL PX2801Z PPE+HIPS (Asia Pacific) PPE+HIPS Unfilled FR V-0 100C |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | ASTM D638 |
Wico Plast Wicoran 57 ABS, High Gloss ApplicationsInjection moldingCharacteristics:High glossAll information provided by Wico Plast, Warenhandelsges. mbH |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | 50 mm/min; ISO 527-1,-2 |
Covestro Bayblend® T65 AT PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Imp.. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | ASTM D638 |
E-Polymers TEKAMID® TA210ST Super Tough PA66, DAM Super ToughnessInformation provided by E-Polymers Co. Ltd. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | 50 mm/min |
Arkema Group Orgalloy® RS 6600 Nylon 66 Alloy, Rigid Grade (Conditioned) RS 66 series, rigid polyamide 66 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional propertie.. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | ISO 527-1 |
Barlog Plastics KEBAFORM C 901 SO POM Copolymer unreinforced, improved wear and friction POMInformation provided by BARLOG plastics GmbH. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | ISO 527-1 |
Barlog Plastics KEBAFORM C 903 LF POM Copolymer unreinforced, improved wear and friction POMInformation provided by BARLOG plastics GmbH. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | 50 mm/min; ISO 527-2 |
BASF Ultraform® N2650 Z2 (LEV) POM Description: Is a POM + PUR, elastomer-modified injection-molding grades with high impact strength for clips, snap and fastening elements, also for components subject to impact stress.Information pr.. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 158 NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Zytel 158 NC010 is an intermediate viscosity PA 612 resin.Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | 50 mm/min |
Polimeri Europa SINKRAL PD G120 ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-09-30 General purpose injection moulding grade. Characteristics: outstanding rigidity very high surface.. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | 50 mm/min |
Arkema Group Kynar® 4000 HD PVDF
(discontinued **) Designation ISO 12086-PVDF-E,GG1N,Q.?E5.I.B.E.C,, ?(6-10)Kynar PVDF are fluorinated thermoplastic homopolymers.Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, high b.. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | SABIC - Japan Method |
SABIC Innovative Plastics NORYL PX2622 PPE+HIPS (Asia Pacific) PPE/HIPS for auto interior |