Barlog Plastics KEBAFORM C 903 LF POM Copolymer unreinforced, improved wear and friction

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced
Manufacturer Barlog Plastics
Trade Name KEBAFORM
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Barlog Plastics KEBAFORM C 903 LF POM Copolymer unreinforced, improved wear and friction.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
POMInformation provided by BARLOG plastics GmbH.
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.20 %
0.20 %
similar to ISO 62 test
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 52.0 MPa
7540 psi
ISO 527-1
Elongation at Yield 8.0 %
8.0 %
ISO 527-1
Tensile Modulus 2.80 GPa
406 ksi
ISO 527-1
Charpy Impact Unnotched NB
NB
ISO 179-1eU
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
ISO 179-1eA
Thermal Properties Metric English Comments
Melting Point 166 °C
331 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Descriptive Properties Value Comments
Resin Type POM
Users viewing this material also viewed the following: