| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 52.0 MPa | 7540 psi | ISO 5272 |
| Polyplastic Armlen® PP GF 20-1EX Polypropylene Copolymer, 20% Glass Fiber Information provided by PolyPlastic Group. |
|||
| Tensile Strength, Yield | 52.0 MPa | 7540 psi | Type I, 50 mm/min; ASTM D 638 |
| SABIC Innovative Plastics Cycoloy® CP8930 PC+ABS (Europe-Africa-Middle East) High heat, PC/ABS for automotive electro plating applications, excellent balance in flow/impactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
| Tensile Strength, Yield | 52.0 MPa | 7540 psi | Type I, 50 mm/min; ASTM D638 |
| SABIC Innovative Plastics Cycoloy® IP1000 PC+ABS (Asia Pacific) IP1000 is a high impact PC/ABS blend developed for the automotive instrument panel business. |
|||
| Tensile Strength, Yield | 52.0 MPa | 7540 psi | 50 mm/min; ISO 527 |
| SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer (Asia Pacific) Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul.. |
|||
| Tensile Strength, Yield | 52.0 MPa | 7540 psi | 50 mm/min; ISO 527 |
| SABIC Innovative Plastics Lexan® ML7647K PC (Asia Pacific) Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque only |
|||
| Tensile Strength, Yield | 52.0 MPa | 7540 psi | ASTM D638 |
| SABIC Innovative Plastics LNP FARADEX NS003 PC+ABS LNP* FARADEX* NS003 is a compound based on PC+ABS resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
| Tensile Strength, Yield | 52.0 MPa | 7540 psi | ASTM D638 |
| Ineos Nova 1280 High Heat Crystal Polystyrene
(discontinued **) Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r.. |
|||
| Tensile Strength, Yield | 52.0 MPa | 7540 psi | 50 mm/min; ASTM D638 |
| SABIC Innovative Plastics Lexan® SLD3000 PC (Asia Pacific) Antistatic colorable/opaque FR PC grade |
|||
| Tensile Strength, Yield | 52.0 MPa @Thickness 3.20 mm |
7540 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
| LG Chemical LUMID HI1202B(W) PA66, High Impact Feature: Injection Molding, PA66, High ImpactApplication: Automotive (Covers)CAS No. 32131-17-2 and 9010-79-1Information provided by LG Chemical |
|||
| Tensile Strength, Yield | 52.0 MPa | 7540 psi | ISO 527-1/-2 |
| Mitsubishi Xantar® MX 1021 FD MX 1021 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
| Tensile Strength, Yield | 52.0 MPa @Thickness 3.20 mm |
7540 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
| LG Chemical LUPOL HR2100D PP+GF17% Description: Injection Molding, PP+GF17%, General PurposeApplication: Electrical, Electronic and Automotive Parts CAS: 9003-07-0 and 165997-17-3Information provided by LG Chemical |
|||
| Tensile Strength, Yield | 52.0 MPa | 7540 psi | Type I, 5 mm/min; ASTM D638 |
| SABIC Innovative Plastics LNP LUBRICOMP RP003 PA 66 LNP* LUBRICOMP* RP003 is a compound based on Nylon 66 resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
| Tensile Strength, Yield | 52.0 MPa | 7540 psi | ISO 527 |
| SABIC Innovative Plastics LNP Stat-kon KS302 Acetal Copoly LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel.This data was supplied by SABIC-IP for the Americas region. |
|||
| Tensile Strength, Yield | 52.0 MPa | 7540 psi | Type I, 50 mm/min; ASTM D 638 |
| SABIC Innovative Plastics Xenoy® 1101 PBT+PC (Asia Pacific) Unreinforced, opaque polycarbonate/polyester alloy. Excellent low temperature impact plus chemical resistance to automotive fluid.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
| Tensile Strength, Yield | 52.0 MPa | 7540 psi | 50 mm/min; ISO 527 |
| SABIC Innovative Plastics Xenoy® CL101 PBT+PC Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
| Tensile Strength, Yield | 52.0 MPa | 7540 psi | 50 mm/min; ISO 527 |
| SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Asia Pacific) Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
| Tensile Strength, Yield | 52.0 MPa | 7540 psi | 50 mm/min; ISO 527 |
| SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Europe-Africa-Middle East) Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
| Tensile Strength, Yield | 52.0 MPa | 7540 psi | Type I, 5 mm/min; ASTM D638 |
| SABIC Innovative Plastics LNP STAT-KON TE002 PU LNP* STAT-KON* TE002 is a compound based on Polyurethane resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
| Tensile Strength, Yield | 52.0 MPa | 7540 psi | 50 mm/min; ASTM D638 |
| Samsung Cheil Industries Infino® LB-1010W PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
| Tensile Strength, Yield | 52.0 MPa | 7540 psi | 50 mm/min; ASTM D638 |
| Samsung Cheil Industries Infino® HP-1011 PC/ABS, Unreinforced Material with superior flowability and small gas generation that can be used in the exterior material of mobile phonesInformation provided by Samsung Cheil Industries. |
|||
| Tensile Strength, Yield | 52.0 MPa | 7540 psi | 5 mm/min; ASTM D638 |
| Samsung Cheil Industries Starex® TF-0956 HI-PMMA Information provided by Samsung Cheil Industries. |
|||
| Tensile Strength, Yield | 52.0 MPa | 7540 psi | Type I, 50 mm/min; ASTM D 638 |
| SABIC Innovative Plastics Valox® V3802 PBT + PC + PET (Asia Pacific) PBT + PC + PET, Mold Release, Flame retardant, Impact Modified, OpaqueThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
| Tensile Strength, Yield | 52.0 MPa | 7540 psi | ASTM D638 |
| Teknor Apex Sinpolene GPP1610 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Glass Fiber Reinforcement, 10% Filler by Weight Features: Good Dimensional Stability; High Heat Resistance; .. |
|||
| Tensile Strength, Yield | 52.0 MPa | 7540 psi | ISO 527-1/-2 |
| Covestro Bayblend® T65 Polycarbonate + ABS General purpose injection molding gradeVicat/B 120 temperature = 120 °Cgood low temperature impact strengthPreprocessingMax. Water content |
|||
| Tensile Strength, Yield | 52.0 MPa @Strain 300 % |
7540 psi @Strain 300 % |
ISO 527-1/-2 |
| Covestro Desmopan® DP 3072D Polyurethane injection molding gradehigh mechanical strengthexcellent abrasion resistancegood wear resistancevery short cycle timesApplicationTechnical partsAs of 1 September 2015, Bayer MaterialScience was sepa.. |
|||
| Tensile Strength, Yield | 52.0 MPa | 7540 psi | |
| BASF Luranyl® KR 2401 Polyphenylene Ether + Styrene-Butadiene Blend, Impact Grade Base grade with a balanced combination of impact strength and stiffness. Uses include: parts of vehicle interiors, air ducts and loudspeaker housings.Data was collected by ISO methods and provided .. |
|||
| Tensile Strength, Yield | 52.0 MPa | 7540 psi | ASTM D638 |
| Ineos Nova 1200 High Heat Crystal Polystyrene Good processing characteristics, High tensile strength and modulus, Excellent clarity, USP Class VIApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radia.. |
|||
| Tensile Strength, Yield | 52.0 MPa | 7540 psi | ASTM D638 |
| Ineos Nova 1204 High Heat Crystal Polystyrene Good processing characteristics, High tensile strength and modulus, Excellent clarity, USP Class VIApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radia.. |
|||
| Tensile Strength, Yield | 52.0 MPa | 7540 psi | 50 mm/min; ASTM D638 |
| Samsung Cheil Industries Infino® HP-1011 PC/ABS, Unreinforced Material with superior flowability and small gas generation that can be used in the exterior material of mobile phonesInformation provided by Samsung Cheil Industries. |
|||
| Tensile Strength, Yield | 52.0 MPa | 7540 psi | ISO 527 |
| Manifattura Cattaneo POM c+PTFE Acetal, PTFE Filled Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||