Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 46.1 MPa @Thickness 3.20 mm |
6680 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical BM662 ABS, Heat Resistance Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical.. |
|||
Tensile Strength, Yield | 46.1 MPa @Thickness 3.20 mm |
6680 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical GPPS 15NF(I) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: Food Container, Merchandise, Artificial Woods, Refrigerator Vegetable Box, PSP, Sheet, Film, etc.CAS: 9003-53-6-5In.. |
|||
Tensile Strength, Yield | 46.1 MPa @Thickness 3.20 mm |
6680 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical HG173 ABS, High Surface Gloss Feature: Injection Molding, High Surface GlossApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Tensile Strength, Yield | 46.1 MPa @Thickness 3.20 mm |
6680 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical HI121U ABS Feature: Injection Molding, Well Balanced Mechanical Properties, Good weatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemic.. |
|||
Tensile Strength, Yield | 46.1 MPa @Thickness 3.20 mm |
6680 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical LG749W ABS, Low Gloss, Heat Resistance Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automotive Interior Housing (Glove Cover, Door S/W Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by.. |
|||
Tensile Strength, Yield | 46.1 MPa @Thickness 3.20 mm |
6680 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOY MP5000AM PC/ABS Description: Injection Molding, PC/ABS, General Purpose, Metal PlatingApplication: Automotive (Exterior), E&E (Housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
Tensile Strength, Yield | 46.1 MPa @Thickness 3.20 mm |
6680 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical RS657L ABS, Chemical Resistance to Cyclopentane, Low Specific Gravity Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Tensile Strength, Yield | 46.1 MPa | 6680 psi | ASTM D638 |
Lendell Parapet GR-00100 PMMA, High Impact |
|||
Tensile Strength, Yield | 46.1 MPa | 6680 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® HA-1011 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 46.1 MPa | 6680 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® HR-0370F ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 46.1 MPa | 6680 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® LX-0981 ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 46.1 MPa | 6680 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® LX-0987EXS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 46.1 MPa | 6680 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® ST-0185 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 46.1 MPa | 6680 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WR-9100SG ASA, Unreinforced Used for solid vinyl door, frame etc.Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 46.1 MPa | 6680 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WR-9370 ASA, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 46.1 MPa | 6680 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® HR-0370F ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 46.1 MPa | 6680 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® LX-0981 ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 46.1 MPa | 6680 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® LX-0987EXS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 46.1 MPa | 6680 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® ST-0185 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 46.1 MPa | 6680 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WR-9100SG ASA, Unreinforced Used for solid vinyl door, frame etc.Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 46.1 MPa | 6680 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WR-9370 ASA, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 46.1 MPa | 6680 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp DBS 8613 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: Good Impact Resistance Uses: Piping Forms: Powder Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 46.1 MPa | 6680 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SRF 3704 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: High Impact Resistance Uses: Fittings Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 46.1 MPa | 6680 psi | ASTM D638 |
Teknor Apex Sinvicomp SRP 9613 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: Good Impact Resistance Uses: Profiles Forms: Granules Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 46.1 MPa @Thickness 3.20 mm |
6680 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Abstron IM14GM ABS Injection Molding Grade High Rigidity, Medium Impact, Good paintabilityInformation provided by Bhansali |
|||
Tensile Strength, Yield | 46.1 MPa @Thickness 3.20 mm |
6680 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Abstron KU603 ABS Heat Resistant High Impact, High RigidityInformation provided by Bhansali |
|||
Tensile Strength, Yield | 46.1 MPa @Thickness 3.20 mm |
6680 psi @Thickness 0.126 in |
Type 1; ASTM D-638 |
Bhansali Engineering Abstron SHF-50+M ABS Injection Molding Grade High Flow High Gloss, Fancy ApplicationsInformation provided by Bhansali |
|||
Tensile Strength, Yield | 46.1 MPa @Thickness 3.20 mm |
6680 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Abstron IM14GM ABS Injection Molding Grade High Rigidity, Medium Impact, Good paintabilityInformation provided by Bhansali |
|||
Tensile Strength, Yield | 46.1 MPa @Thickness 3.20 mm |
6680 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Abstron KU603 ABS Heat Resistant High Impact, High RigidityInformation provided by Bhansali |
|||
Tensile Strength, Yield | 46.1 MPa @Thickness 3.20 mm |
6680 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical SG175G ABS, Super Surface Gloss, High Flow Feature: Injection Molding, Super Surface Gloss, High FlowApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical |