Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 37.0 MPa | 5370 psi | 4.0 mm thick, 10.0 mm wide molded rod; ISO 527 |
Premix Thermoplastics PRE-ELEC® ESD 7200 PRE-ELEC ESD 7200 is a static dissipative thermoplastic compound based on PC/ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7200 has been developed for inj.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Ineos H00M-00 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Extrusion; ThermoformingFeatures: High melt strength, Enhanced flow, Medium-term heat agingComplies with FDA specification, Title 21, CFR 177.1520.Typical applications.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Flint Hills H0500HN Polypropylene Homopolymer Features: Nucleated and long term heat aging (LTHA). Product does not contain animal derived components. Phthalate-free.Applications: Injection molding: medical partsInformation Provided by Flint .. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Flint Hills P4C5B-075 Homopolymer Polypropylene Homopolymer, and FDA compliant.Features: Nucleated, antistat, and controlled rheology.Applications: Injection molding: tape extrusion and closures.Former Huntsman polypropylene products are now prod.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Flint Hills P4C5B-076 Homopolymer Polypropylene Homopolymer, and FDA compliant.Features: Nucleated, antistat, and controlled rheology.Applications: Injection molding: cutlery and closuresFormer Huntsman polypropylene products are now produced by .. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Flint Hills P4G4Z-011 Homopolymer Polypropylene Homopolymer, UL certified, USP Class VI certified, and FDA compliant.Features: Applications: Injection molding: general purpose, extruded decorative ribbon, and extruded fiber.Former Huntsman polypr.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
IRPC Polimaxx Polene 1102H Polypropylene Homopolymer CHARACTERISTICS: GOOD STIFFNESS, GOOD EXTRUDABILITY, HIGH IMPACTAPPLICATIONS: MONOFILAMENT/YARN/SHEET EXTRUSION FOR THERMOFORMINGBLOW MOLDING AND INJECTION MOLDING FOR ROPESCOARSE TEXTILE FOR JUMBO .. |
|||
Tensile Strength, Yield | 37.0 MPa @Strain 0.200 %, Temperature 1095 °C |
5370 psi @Strain 0.200 %, Temperature 2003 °F |
|
Haynes 263® alloy, cold rolled sheet, solution treated and aged Very good aged strength properties, excellent fabrication characteristics when annealed, excellent intermediate temperature tensile ductility, is not normally subject to strain age cracking, excelle.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp KZL34 POM LNP* Lubricomp* KZL34 is a compound based on Acetal resin containing Milled Glass and PTFE. Characteristic of this grade is Internally Lubricated.This data was supplied by SABIC-IP for the Americas.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA 12 (Asia Pacific) LNP* Lubricomp* SP003 is a compound based on Nylon 12 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp ZI001 PPO LNP* Lubricomp ZI001 is a compound based on Modified PPO containing Silicone. Characteristics are internally lubricated.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP ZI001XXX PPE+PS (Asia Pacific) LNP* Lubricomp* ZI001XXX is a compound based on PPE+PS Blend resin. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON WS002I PBT LNP* STAT-KON* WS002I is a compound based on PBT resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, High Impact. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP AX08306 ABS LNP* THERMOCOMP* AX08306 is a compound based on ABS resin containing Proprietary Filler(s). Added feature of this grade is: Platable. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP AX08306 ABS (Asia Pacific) LNP* Thermocomp* AX08306 is a compound based on Acrylonitrile Butadiene Styrene resin containing Mineral. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PN235 PPE+PS (Asia Pacific) Plating grade, primarily automotive applications. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT (Asia Pacific) LNP* Lubricomp* WBL36L is a compound based on Polybutylene Terephalate resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ISO 527 |
SABIC Innovative Plastics LNP Stat-loy W3000 PBT LNP STAT-LOY* W3000 is a compound based on Polybutylene Terephalate resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americ.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | SABIC - Japan Method |
SABIC Innovative Plastics Noryl EUN0240 PPE+HIPS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Teknor Apex Sinpolene TPP1040 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Talc Filler, 40% Filler by Weight Uses: Automotive Applications; Housings Forms: Pellets Processing Method: Injection .. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
UBE UBESTA® P3014UMX Powder Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ISO 527-2 |
Total PPH 12020 Polypropylene Homopolymer, Injection Molding Polypropylene PPH 12020 is a clarified high fluidity homopolymer with a melt flow index of 60 g/10 min.Polypropylene PPH 12020 has been designed with a very high stiffness and an outstanding transpa.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ISO 527-2 |
Denka MALECCA K-600 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Aclo Accucomp ABS ABS801L Medium Impact Grade |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Aclo Accuguard Polypropylene HP0362V0CSL Homopolymer Flame Retardant Copper Stabilized |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | 50 mm/min |
Arkema Group Rilsan® AECN TL Nylon 12, Cable Sheathing Grade (Conditioned) Designation ISO 1874-PA12,KHL,14-010Extrusion grade for the sheathing of wires and cables. Available colors: natural and orange. Heat and light stabilized.Low melt viscosity. High speed extrusion. V.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0339T10L1 Talc Reinforced |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ISO 527 |
SABIC Innovative Plastics LNP Lubricomp CI001 PS (Asia Pacific) LNP* Lubricomp* CI001 is a compound based on Polystyrene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pa.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Ineos H35G-01 Polypropylene Homopolymer